| 热循环对Cu-Zn-Al合金热弹性马氏体转变的影响 |
| 李健纯;G.S.Ansell |
| 中南矿冶学院;美国莱塞尔多科性理工学院;院长 |
|
| EFFECT OF THERMAL CYCLING ON THERMOELASTIC MARTENSITIC TRANSFORMATION IN A Cu-Zn-Al ALLOY |
| Li Jianchun (Central South Institute of Mining and Metallurgy; Changsha); G. S. Ansell (Rensselaer Polytechnic Institute; Troy; N. Y.; U. S. A.) |
引用本文:
李健纯;G.S.Ansell. 热循环对Cu-Zn-Al合金热弹性马氏体转变的影响[J]. 金属学报, 1982, 18(5): 544-639.
,
.
EFFECT OF THERMAL CYCLING ON THERMOELASTIC MARTENSITIC TRANSFORMATION IN A Cu-Zn-Al ALLOY[J]. Acta Metall Sin, 1982, 18(5): 544-639.
1 Horace P.; Massalski, T. B., Trans. Metall Soc. AIME, 230 (1964) , 1662. 2 Kajiwara, S., Trans. Natl. Res. Inst. Met. (Jpn), 18 (1967) , No. 6, 220. 3 Schroeder, T. A.; Cornelis, I; Wayman, C. M., Metall. Trans., 7A (1976) , 535. 4 Rapacioli, R.; Chandrassekaran, M.; Delaey, L., Shape Memory Effects in Alloys, Plenum Press, New York, 1975, p. 365. 5 Easterling, K. E.; Miekk-oja, H. M., Acta Metall., 15 (1967) , 1133. |
|