Please wait a minute...
金属学报  1983, Vol. 19 Issue (3): 77-83    
  论文 本期目录 | 过刊浏览 |
Fe-Cu-C和Fe-Cu-Co-C熔体的热力学性质
彭瑞伍;汪光裕;张俊岳
中国科学院上海冶金研究所;中国科学院上海冶金研究所;中国科学院上海冶金研究所
THERMODYNAMIC PROPERTIES OF Fe-Cu-C AND Fe-Cu-Co-C MELTS
by PENG Ruiwu; WANG Guangyu; ZHANG Junyue (Shanghai Institute of Metallurgy; Academia Sinica)
引用本文:

彭瑞伍;汪光裕;张俊岳. Fe-Cu-C和Fe-Cu-Co-C熔体的热力学性质[J]. 金属学报, 1983, 19(3): 77-83.
, , . THERMODYNAMIC PROPERTIES OF Fe-Cu-C AND Fe-Cu-Co-C MELTS[J]. Acta Metall Sin, 1983, 19(3): 77-83.

全文: PDF(481 KB)  
摘要: 本文测得碳在Fe-Cu-C和Fe-Cu-Co-C系中的溶解度和分层数据,计算这些体系中Cu和Fe的活度系数以及碳对Cu和Fe活度系数的影响。结果表明,随着体系中碳量的增加,相应地Cu活度系数增加,而Fe活度系数减少。在这些数据的基础上,还计算了Fe-Cu-C系的一级、二级活度相互作用系数,等活度时自由能相互作用系数和焓相互作用系数,并估计了Cu量对碳溶解过剩焓的影响。计算结果与其它已报道的Fe-j-C系相比较,发现这些热力学性质与原子序数之间有一定的规律。
Abstract:The solubility of C and the activity coefficient of Cu and Fc in Fc-Cu-C and Fc-Cu-Co-C systems at 1550℃ were calculated. The results indicate that the activity coefficient of Cu increases and of Fe decreases with the increase of C content. On the basis of data obtained, the first and second order activity interaction coefficients in Fc-Cu-C systcm and interaction coefficients of free energy or enthalpy at constant activity as well as the partial molar heat of mixing of C affected by the Cu content were estimated. Compared with the thermodynamic functions of other Fc-j-C systems after previous works, the regular correlation between these thermodynamic properties and the atomic number of j element seems to be noticeable.
收稿日期: 1983-03-18     
1 Iwase, K., Okamoto, M., Amemiya, T.; Sci. Rep. Tohoku Imp. Univ., 26 (1937) , 618.
2 Koros, J.; Chipman, J., Trans. AIME, 206 (1956) , 1102.
3 Schenck, H., Arch. Eisenhuettenwes., 32 (1961) , 123.
4 彭瑞伍,邹元爔,金属学报,6(1963) ,111.
5 Mathien, G., Scr. Metall., 7 (1973) , 421.
6 Morris, J. P.; Zellans, G. R., Trans. AIME, 206 (1956) , 1086.
7 Foo, E. H.; Lupis, C. H. P., Metall. Trans., 3 (1972) , 2125.
8 Lupis, C. H. P., Metall. Trans., 5 (1974) , 1919.
9 彭瑞伍;汪光裕;张俊岳,待发表.
10 魏寿昆,冶金过程热力学,上海科技出版社,1980,p.231.a