| 一种简单六角点阵的缺陷结构 |
| 苗柏和;孟宪英;赵伯麟 |
| 北京钢铁学院;北京钢铁学院;北京理化测试中心;北京钢铁学院 |
|
| ONE KIND OF FAULT STRUCTURE OF SIMPLE HEXAGONAL LATTICE |
| MIAO Baihe; MENG Xianying; ZHAO Bolin (Beijing University of Iron and Steel Technology) |
引用本文:
苗柏和;孟宪英;赵伯麟. 一种简单六角点阵的缺陷结构[J]. 金属学报, 1983, 19(5): 95-101.
,
,
.
ONE KIND OF FAULT STRUCTURE OF SIMPLE HEXAGONAL LATTICE[J]. Acta Metall Sin, 1983, 19(5): 95-101.
1 Arnfelt, H.; Westgren, A., Strukturbericht, 3 (1937) , 364. 2 Forsyth, J. B.; Veiga, L. M. d' Alte Da, Acta Cryst. 15 (1962) , 543. 3 Raman, A., Z. Metallk. 57 (1966) , 301. 4 Sinha, A. K.; Buckley, R. A.; Hume-Rothery, W., J. Iron Steel. Inst., 205 (1967) , 191. 5 Sinha, A. K.; Hume-Rothery, W., ibid., 205 (1967) , 1145. 6 Kohei Yagisawa; Hiroshi Fujita, Jpn. J. Appl. Phys., 6 (1967) , 826. 7 Lars Stenberg; Sten Andersson, J. Solid State Chem., 28 (1979) , 269. 8 Makoto Hirabayashi; Kenji Hiraga; Daisuke Shindo; Tadashi Yamamoto, Sci Rep. Res. Inst., Tohoku Uni. Ser. A29 Suppl. 1, (1981) , 1. 9 赵伯麟;苗柏和;陈国良,金属学报,17 (1981) ,386. 10 陈国良,谢锡善,倪克铨;徐志超;王迪,金属学报,17 (1981) ,1. 11 蔡玉林;郑运荣,金属学报,18 (1982) ,30.5 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|