多元低合金钢马氏体相变热力学
李麟;徐祖耀
山东工学院;上海交通大学
THERMODYNAMICS OF MARTENSITIC TRANSFORMATION IN LOW ALLOYING MULTICOMPONENT STEELS
by LI Lin (Shandong Institute of Technology); XU Zuyao (T. Y. Hsu) (Shanghai Jiaotong University) (Manuscript received 21 March; 1983)
引用本文:

李麟;徐祖耀. 多元低合金钢马氏体相变热力学[J]. 金属学报, 1984, 20(2): 112-117.
, . THERMODYNAMICS OF MARTENSITIC TRANSFORMATION IN LOW ALLOYING MULTICOMPONENT STEELS[J]. Acta Metall Sin, 1984, 20(2): 112-117.

全文: PDF(419 KB)  
摘要: 在以往工作基础上,提出多元低合金钢马氏体相变热力学方程式: 用数学和实验方法证实了这个计算式,并指出联系动力学方程后,可用以计算淬硬钢的残余奥氏体量。
Abstract:An equation for calculating △G intthe martensitic trasformation of the low alloying multicomponent steels has been suggested as: being proved by the mathematic analyses and verified by the practical data of 20CrMnTi steel. The amount of the retained austenite in a hardened steel can be estimated by the equation together with the kinetic formula.
收稿日期: 1984-02-18     
1 徐祖耀,金属学报,15(1979) ,329.
2 徐祖耀,马氏体相变与马氏体,科学出版社,1980,p.246.
3 徐祖耀,金属学报,16(1980) ,426.
4 Wada, T.; Wada, H.; Elliott, J. F.; Chipman, J., Metall. Trans., 2(1971) , 2199.
5 Swartz, J. C., Trans. Metall.Soc. AIME, 245(1969) , 1083.
6 Kaufman, L.; Clougherty, E. V.; Weiss, R. J., Acta Metall., 11(1963) , 323.
7 Kaufman, L.; Cohen, M., Trans. AIME, 206(1956) , 1393.
8 徐祖耀,马氏体相变与马氏体,科学出版社,1980,p.260.
9 Davies, R. G.; Magee, C. L., Metall. Trans., 2(1971) . 1939.
10 日本学术振兴会制钢第19委员会,铁纲合金元素,诚文堂新光社,1966,p.670.
11 三本木贡治,大谷,铁钢,47(1961) ,841.
12 Nelson, E. C., Trans. Metall. Soc. AIME, 277(1963) , 189.
13 徐祖耀,金属材料热力学,科学出版社,1981,p.304.
14 热处理手册编委会,热处理手册,第四分册,机械工业出版社,1978,附44.
No related articles found!