| Ni-Mo-Al-V四元定向共晶的条带组织 |
| 张玉生;于洋;唐亚俊;张静华;王素坤;胡壮麒 |
| 中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所 |
|
| A NOTE ON BAND STRUCTURE IN DIRECTIONALLY SOLIDIFIED EUTECTIC ALLOY OF Ni-Mo-Al-V SYSTEM |
| by ZHANG Yusheng; YU Yang; TANG Yajun; ZHANG Jinghua; WANG Sukun; HU Zhuangqi (Institute of Metal Research; Academia Sinica; Shenyang) (Manuscript received 27 May; 1983) |
引用本文:
张玉生;于洋;唐亚俊;张静华;王素坤;胡壮麒. Ni-Mo-Al-V四元定向共晶的条带组织[J]. 金属学报, 1984, 20(2): 118-123.
,
,
,
,
,
.
A NOTE ON BAND STRUCTURE IN DIRECTIONALLY SOLIDIFIED EUTECTIC ALLOY OF Ni-Mo-Al-V SYSTEM[J]. Acta Metall Sin, 1984, 20(2): 118-123.
1 Carruthers, J. R.; Witt, A. F., Crystal Growth and Characterization, Proc. of ISSCG 2, Springschool, Japan, Eds. Ueda, R.; Mullin, J.B., North-Holland, Amsterdam, 1975, p. 107. 2 Smith, V. G.; Tiller, W. A.; Rutter, J. W., Can. J. Phys., 33(1955) , 723. 3 Flemings, M. C., Solidification Processing, McGraw-Hill, New York, 1974, p. 53. 4 Cole, G. S., Solidification, ASM, Metal Park, Ohio, 1971, p. 201. 5 Neff, M. A.; Rickinson, B. A.; Young, K. P.; Flemings, M. C., Metall. Trans., 9B(1978) , 469. 6 Nakagawa, Y. G.; Murakami, K.; Ohotomo, A.; Saiga, Y., Trans. Iron Steel Inst. Jpn., 20 (1980) ,614. 7 Hansen, M., Constitution of Binary Alloys, McGraw-Hill, New York, 1958, p. 1055. 8 Sprenger, M.; Richter, H.; Nickl, J. J., Mater. Sci., 11(1976) , 2075. 9 Pearson, D. D.; Lemkey, F. D., Solidification and Casting of Metals, Proc. of an Int. Conf. on Solidification, Sheffield, England, 1979, p. 526. 10 Lemkey, F. D., Superalloys: Metallurgy and Manufacture, Proc. of the 3rd Int. Symp., Seven Springs, PA., Eds. Kear, B. H.; Muzyka, D. R.; Tien, J. K. et al., Claitor's Publ., Baton Rouge, 1976, p. 321. 11 Nakagawa, Y. G.; Ohotomo, A.; Saiga, Y.; Memoto, M., Superalloys 1980, Proc. of the Fourth Int. Symp. on Superalloys, Seven Springs, PA., Eds. Tien, J. K.; Wlodek, S. T.; Morrow, H. Ⅲ; et al., ASM, Metals Park, Ohio, 1980, p. 267. 12 傅恒志,高温合金非平衡状态的凝固特性,全国特种铸造及有色合金第一届学术报告会论文集,1980.H |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|