| Al-Si共晶合金变质机理的探讨(Ⅱ)——Si相的不平衡度与形貌的关系 |
| 张启运;刘淑祺;胡佳 |
| 北京大学化学系;北京大学化学系;北京大学化学系 |
|
| THE MODIFICATION OF Si PHASE IN A1-Si EUTECTIC ALLOYS(Ⅱ)——Relationship between Unequilibrium Degree of Si Phase and its Appearance |
| by ZHANG Qiyun; LIU Shuqi; HU Jia (Dept. of Chemistry; Peking University)(Manuscript received 1 September; 1982; revised manuscript 23 August; 1983) |
引用本文:
张启运;刘淑祺;胡佳. Al-Si共晶合金变质机理的探讨(Ⅱ)——Si相的不平衡度与形貌的关系[J]. 金属学报, 1984, 20(2): 138-218.
,
,
.
THE MODIFICATION OF Si PHASE IN A1-Si EUTECTIC ALLOYS(Ⅱ)——Relationship between Unequilibrium Degree of Si Phase and its Appearance[J]. Acta Metall Sin, 1984, 20(2): 138-218.
1 Day, M. G.;. Hellawell, A., J. Inst. Met., 95 (1967) , 377. 2 郑朝贵;姚连克;张启运,金属学报,18(1982) ,661. 3 张启运;郑朝贵;韩万书,金属学报,17(1981) ,130. 4 Phrogmen, G., J. Inst. Met., 77(1950) , 498. 5 张启运;刘淑祺;樊晓红,金属学报,18(1982) ,581. |
|