| 非晶合金低频损耗和频率的非线性关系来源的探讨 |
| 张延忠 |
| 上海钢铁研究所 |
|
| A NOTE ON BEHAVIOUR OF NON-LINEAR DEPENDENCE OF LOW FREQUENCY LOSS UPON FREQUENCY FOR AMORPHOUS ALLOYS |
| ZHANG Yanzong (Shanghai Iron and Steer Research Institute) (Manuscript received 24 February; 1983; revised manuscript 5 July; 1983) |
引用本文:
张延忠. 非晶合金低频损耗和频率的非线性关系来源的探讨[J]. 金属学报, 1984, 20(3): 214-220.
.
A NOTE ON BEHAVIOUR OF NON-LINEAR DEPENDENCE OF LOW FREQUENCY LOSS UPON FREQUENCY FOR AMORPHOUS ALLOYS[J]. Acta Metall Sin, 1984, 20(3): 214-220.
1 佐佐木堂;桂川茂彦,电气学会论文志,97-A(1977) ,601. 2 Sasaki, T; Hosoe, H., IEEE Trans. Magn., MAG-14 (1978) , 779. 3 Fujimori, H.; Yoshimoto, H.; Masumoto, T., J. Appl. Phys., 52 (1981) , 1893. 4 Washko, S.D.; Osborn, M.L.; Veeraraghaven, W.G., ibid., 52 (1981) , 1899. 5 Sakaki, Y., IEEE Trans. Magn., MAG-16 (1980) , 569. 6 Ferrari, G., Portesell, J. L.; Vergne, R., ibid., MAG-14 (1978) , 764. 7 Ne'el, L., J. Phys. Radium, 11 (1950) , 49. 8 Haller, T. R.; Kramer, J. J., J. Appl. Phys., 41 (1970) , 1034. 9 Pry, R. H.; Bean, C. P., ibid., 29 (1958) , 532. 10 Haller, T. R.; Kramer, J.J., ibid., 41 (1970) , 1036. 11 Sharp, M.R.G.; Horner, J.T., J. Phys. D: Appl. Phys., 6 (1973) , 1835. 12 Mohri, K.; Satoh, Y.; Fujimoto, T., IEEE Trans, Magn., MAG-12 (1976) , 849. 13 29 (1970) , 770. 14 郭贻诚,铁磁学,高等教育出版社,北京,1965,p.355. 15 北京大学物理系,铁磁学编写组,铁磁学,科学出版社,北京,1976年,p.211. 16 Sakaki, Y.; Imagi, I., IEEE Trans. Magn., MAG-17 (1981) , 1478. 17 张延忠,科学通报(待发表). |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|