| 关于铝钎焊冶金过程的一个问题 |
| 张启运;刘淑祺 |
| 北京大学化学系;北京大学化学系 |
|
| A PROBLEM ON METALLURGICAL PROCESS DURING ALUMINUM BRAZING——Wish to Discuss with Mr. CHEN Genbao and Others |
| ZHANG Qiyun; LIU Shuqi (Dept. of Chemistry; Beijing University) (Manuscript received 5 September; 1983) |
引用本文:
张启运;刘淑祺. 关于铝钎焊冶金过程的一个问题[J]. 金属学报, 1984, 20(3): 280-282.
,
.
A PROBLEM ON METALLURGICAL PROCESS DURING ALUMINUM BRAZING——Wish to Discuss with Mr. CHEN Genbao and Others[J]. Acta Metall Sin, 1984, 20(3): 280-282.
1 张启运,刘淑祺,金属学报,17(1981) ,300. 2 陈根宝;吴锦华;李戈扬,金属学报,20(1984) . 3 Hansen, M., Constitution of Binary Alloys, 2nd ed., McGraw-Hill, New York, 1958, p. 133. 4 郑朝贵;姚连克;张启运,金属学报,18(1982) ,661. 5 张启运;刘淑祺;胡佳,金属学报,20(1984) ,A141 |
|