Please wait a minute...
金属学报  1984, Vol. 20 Issue (4): 340-344    
  论文 本期目录 | 过刊浏览 |
磁场和张力退火对金属玻璃Fe_(78)Si_(10)B_(12)磁性的影响
陈笃行
冶金工业部钢铁研究总院
EFFECT OF MAGNETIC FIELD-AND TENSIONANNEALING ON MAGNETIC PROPERTIES OF AN Fe_(78)Si_(10)B_(12) METALLIC GLASS
CHEN Duxing (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 25 May; 1983; revised manuscript 20 October; 1983)
引用本文:

陈笃行. 磁场和张力退火对金属玻璃Fe_(78)Si_(10)B_(12)磁性的影响[J]. 金属学报, 1984, 20(4): 340-344.
. EFFECT OF MAGNETIC FIELD-AND TENSIONANNEALING ON MAGNETIC PROPERTIES OF AN Fe_(78)Si_(10)B_(12) METALLIC GLASS[J]. Acta Metall Sin, 1984, 20(4): 340-344.

全文: PDF(325 KB)  
摘要: 通过磁场和张力退火对金属玻璃Fe_(78)Si_(10)B_(12)磁导率影响的研究,发现存在磁化感生和应变感生的两种磁各向异性,二者分别具有正值和负值的各向异性常数。
Abstract:A study was made of the effect of magnetic field-and tension-annealing under temperature below T_c on the permeability of an Fe_(78)Si_(10)B_(12) metallic glass. Two anisotropies induced by magnetization and by strain were observed with K_(um)>0 and K_(us)<0 respectively. The variations of K_(um) and K_(us) with the magnetization and the strain respectively during anneals are reversible basically.
收稿日期: 1984-04-18     
1 Luborsky, F. E.; Becker, J. J., IEEE Trans. Magn., MAG-15(1979) , 1939.
2 Narita, K.; Fukunaga, H.; Yamasaki, J.; Hara, K., J. Magn. Magn. Mater., 19 (1980) , 145.
3 Mizoguchi, T.; Hatta, S.; Kato, H.; Arai, H.; Maeda, K.; Akutsu, N., IEEE Trans. Magn., MAG-16 (1980) , 1147.
4 Mitchell, M. A.; Cullen, J. R.; Abbundi, R.; Clark, A.; Savage, H., J. Appl. Phys., 50 (1979) , 1627.
5 O' Handley, R. C., Phys. Rev., B18 (1978) , 930.
No related articles found!