| 磁场和张力退火对金属玻璃Fe_(78)Si_(10)B_(12)磁性的影响 |
| 陈笃行 |
| 冶金工业部钢铁研究总院 |
|
| EFFECT OF MAGNETIC FIELD-AND TENSIONANNEALING ON MAGNETIC PROPERTIES OF AN Fe_(78)Si_(10)B_(12) METALLIC GLASS |
| CHEN Duxing (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 25 May; 1983; revised manuscript 20 October; 1983) |
引用本文:
陈笃行. 磁场和张力退火对金属玻璃Fe_(78)Si_(10)B_(12)磁性的影响[J]. 金属学报, 1984, 20(4): 340-344.
.
EFFECT OF MAGNETIC FIELD-AND TENSIONANNEALING ON MAGNETIC PROPERTIES OF AN Fe_(78)Si_(10)B_(12) METALLIC GLASS[J]. Acta Metall Sin, 1984, 20(4): 340-344.
1 Luborsky, F. E.; Becker, J. J., IEEE Trans. Magn., MAG-15(1979) , 1939. 2 Narita, K.; Fukunaga, H.; Yamasaki, J.; Hara, K., J. Magn. Magn. Mater., 19 (1980) , 145. 3 Mizoguchi, T.; Hatta, S.; Kato, H.; Arai, H.; Maeda, K.; Akutsu, N., IEEE Trans. Magn., MAG-16 (1980) , 1147. 4 Mitchell, M. A.; Cullen, J. R.; Abbundi, R.; Clark, A.; Savage, H., J. Appl. Phys., 50 (1979) , 1627. 5 O' Handley, R. C., Phys. Rev., B18 (1978) , 930. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|