氧离子注入使晶态Al转变为非晶态Al_2O_3的研究 |
孙树滋 |
东北工学院 |
|
TRANSITION FROM CRYSTALLINE Al TO AMORPHOUS Al_2O_3 BY O~+-IMPLANTATION |
SUN Shuzi (Northeast Institute of Technology; Shenyang) (Manuscript received 28 March; 1983; revised manuscript 8 October; 1983) |
引用本文:
孙树滋. 氧离子注入使晶态Al转变为非晶态Al_2O_3的研究[J]. 金属学报, 1984, 20(4): 358-361.
.
TRANSITION FROM CRYSTALLINE Al TO AMORPHOUS Al_2O_3 BY O~+-IMPLANTATION[J]. Acta Metall Sin, 1984, 20(4): 358-361.
1 Borders, J. A.; Cullis, A.G; Poate, J.M., Applications of Ion Beams to Materials, Ed. Carter, G., Phys. Conf. Ser. 28, 1976, Chapt. 5, p.204. 2 Myers, S.M., J. Vac. Sci. Technol., 17 (1980) , 310. 3 Poate, J.M., J. Vac. Sci. Technol., 15 (1978) , 1636. 4 Carter, G.; Grant, W.A., Ion Implantation of Semiconductors, Edward Arnold, London, 1976. 5 Grant, W.A., J. Vac. Sci. Technol., 15(1978) , 1644. |
|