| 热盐腐蚀对一种镍基高温合金持久性能的影响 |
| 魏翔云;郝惠清;肖耀天 |
| 中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所 |
|
| EFFECT OF HOT SALT CORROSION ON CREEP RUPTURE BEHAVIOUR OF A Ni-BASE SUPERALLOY |
| WEI Xiangyun; HAO Huiqing; XIAO Yaotian (Institute of Metal Research; Academia Sinica; Shenyang)(Manuscript received 20 November; 1982; revised manuscript 22 March; 1983) |
引用本文:
魏翔云;郝惠清;肖耀天. 热盐腐蚀对一种镍基高温合金持久性能的影响[J]. 金属学报, 1984, 20(5): 365-370.
,
,
.
EFFECT OF HOT SALT CORROSION ON CREEP RUPTURE BEHAVIOUR OF A Ni-BASE SUPERALLOY[J]. Acta Metall Sin, 1984, 20(5): 365-370.