| 热等静压处理对铸造镍基高温合金力学性能的影响 |
| 黄荣芳;唐亚俊;李英敖;郭建亭 |
| 中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所 |
|
| INFLUENCE OF HIP ON MECHANICAL PROPERTIES OF THREE Ni-BASE SUPERALLOYS |
| HUANG Yunfang; TANG Yiajun; LI Yingao; GUO Jianting (Institute of Metal Research; Academia Sinica; Shenyang) (Manuscript received 6 August; 1983) |
引用本文:
黄荣芳;唐亚俊;李英敖;郭建亭. 热等静压处理对铸造镍基高温合金力学性能的影响[J]. 金属学报, 1984, 20(5): 414-421.
,
,
,
.
INFLUENCE OF HIP ON MECHANICAL PROPERTIES OF THREE Ni-BASE SUPERALLOYS[J]. Acta Metall Sin, 1984, 20(5): 414-421.