| 二维二元系统在某些相图研究中的应用 |
| 杜宜瑾;陈立溁;严祖同 |
| 安徽师范大学;安徽师范大学;安徽师范大学 |
|
| APPLICATION OF TWO-DIMENSIONAL BINARY SYSTEM TO STUDY CERTAIN PHASE DIAGRAMS |
| DU Yijing; CHEN Lirong; YAN Zutong (Department of Physics; Anhui Normal University; Wuhu) (Manuscript received 16 May; 1983; revised manuscript 23 September; 1983) |
引用本文:
杜宜瑾;陈立溁;严祖同. 二维二元系统在某些相图研究中的应用[J]. 金属学报, 1984, 20(5): 422-430.
,
,
.
APPLICATION OF TWO-DIMENSIONAL BINARY SYSTEM TO STUDY CERTAIN PHASE DIAGRAMS[J]. Acta Metall Sin, 1984, 20(5): 422-430.
1 Collins, R. , Proc. Phys. Soc. , 83 (1964) , 553. 2 杜宜瑾;陈立溁;严祖同,物理学报,31(1982) ,939. 3 杜宜瑾;陈立溁;严祖同,物理学报,32(1983) .96. 4 #121 |
|