| LaNi_xAl_y合金吸氢性能的研究 |
| 钱久信;赵黎明;郑朝贵;叶于浦 |
| 北京大学化学系;北京大学化学系;北京大学化学系;北京大学化学系 |
|
| HYDROGEN ABSORPTION OF LaNi_xAl_y ALLOYS |
| QIAN Jiuxin; ZHAO Liming; ZHENG Chaogui; YE Yupu (Department of Chemistry; Peking University. Beijing) (Manuscript received 15 September; 1983; revised manuscript 9 February; 1984) |
引用本文:
钱久信;赵黎明;郑朝贵;叶于浦. LaNi_xAl_y合金吸氢性能的研究[J]. 金属学报, 1984, 20(6): 423-428.
,
,
,
.
HYDROGEN ABSORPTION OF LaNi_xAl_y ALLOYS[J]. Acta Metall Sin, 1984, 20(6): 423-428.
1 Van Mal, H. H.; Buschow, K. H. J.; Miedema, A. R., J. Less-Common Met., 35 (1974) , 65. 2 Mendelsohn, M. H.; Gruen, D. M.; Dwight, A. E., The Rare Earth in Modern Science and Technology, Eds. McCarthy, G. J.; Rhyne, J. J., Plenum Press, New York, 1978, p. 25. 3 Achard, J. C.; Percheron-Guegan, A.; Diaz, H.; Briaucourt, F.; Demany, F., Hydrogen in Metall, Vol.2, Proc. of the 2nd Int. Congress, Held at Paris, June 1977, Behalf of the Int. Association for Hydrogen Energy, Paris, 1977, p. 1El2. 4 Dwight, A. E., The Rare Earth in Modern Science and Technology, Eds. McCarthy, G. J.; Rhyne, J. J., Plenum Press, New York, 1978, p. 325.+ |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|