| 上限元法求解轴对称挤压变形力 |
| 许其亮;史文华 |
| 西安冶金建筑学院;西安冶金建筑学院 |
|
| THE UPPER BOUND ELEMENT TECHNIQUE OF SOLVING AXISYMMETRIC EXTRUSION FORCE |
| XU Qiliang;SHI Wenhua Xi'an Institute of Metallurgy and Construction Engineering |
引用本文:
许其亮;史文华. 上限元法求解轴对称挤压变形力[J]. 金属学报, 1985, 21(2): 102-110.
,
.
THE UPPER BOUND ELEMENT TECHNIQUE OF SOLVING AXISYMMETRIC EXTRUSION FORCE[J]. Acta Metall Sin, 1985, 21(2): 102-110.
1 Slater,R.A.C.,Engineering Plasticity Theory and Application to Metal Forming Proceses,Macmillan Press Ltd,London,1977,p.394,398. 2 木内学;村田良美,塑性(?)加工,22(1981) ,495. 3 #12 4 Johnson,W.;Kudo,H.,The Mechanics of Metal Extrusion,Manchester University Press,1962,p.60,102. 5 徐秉业;陈森灿,塑性理论简明教程,清华大学出版社,1981,p.283,304. 6 西山卯二郎,塑性加工学,养贤堂发行,1977,p.268. 7 汪大年,金属塑性成形原理,机械工业出版社,1982,p.235. 8 杨守山,有色金属塑性加工学,冶金工业出版社,1982,p.240. 9 重有色金属材料加工手册编写组,重有色金属材料加工手册,(第四分册),冶金工业出版社,1980,p.19. 10 许其亮,未发表资料,1983. |
|