金属学报  1985, Vol. 21 Issue (2): 102-110    
  论文 本期目录 | 过刊浏览 |
上限元法求解轴对称挤压变形力
许其亮;史文华
西安冶金建筑学院;西安冶金建筑学院
THE UPPER BOUND ELEMENT TECHNIQUE OF SOLVING AXISYMMETRIC EXTRUSION FORCE
XU Qiliang;SHI Wenhua Xi'an Institute of Metallurgy and Construction Engineering
引用本文:

许其亮;史文华. 上限元法求解轴对称挤压变形力[J]. 金属学报, 1985, 21(2): 102-110.
, . THE UPPER BOUND ELEMENT TECHNIQUE OF SOLVING AXISYMMETRIC EXTRUSION FORCE[J]. Acta Metall Sin, 1985, 21(2): 102-110.

全文: PDF(521 KB)  
摘要: 根据上限定理之应用——上限元法,设计了符合金属流动规律的空间截锥刚性基元体的上限模式,解决了轴对称挤压变形力的上限估计问题.经验证,用所得公式计算的上限解很接近真实解,使挤压力的计算精度大为提高.
Abstract:The design of a mode of the spatially truncated rigid cone element to con-form with the metal flow was made by the application of the upper bound the-ory-upper bound element technique.The problem to estimate the upper bound ofaxisymmetric extrusion deformation force may be solved consequently.Solutioncalculated by this mode after trial done on practice is in agreement with the actu-al one and the precision of calculation of the extrusion force seems to be muchimproved.
收稿日期: 1985-02-18     
1 Slater,R.A.C.,Engineering Plasticity Theory and Application to Metal Forming Proceses,Macmillan Press Ltd,London,1977,p.394,398.
2 木内学;村田良美,塑性(?)加工,22(1981) ,495.
3 #12
4 Johnson,W.;Kudo,H.,The Mechanics of Metal Extrusion,Manchester University Press,1962,p.60,102.
5 徐秉业;陈森灿,塑性理论简明教程,清华大学出版社,1981,p.283,304.
6 西山卯二郎,塑性加工学,养贤堂发行,1977,p.268.
7 汪大年,金属塑性成形原理,机械工业出版社,1982,p.235.
8 杨守山,有色金属塑性加工学,冶金工业出版社,1982,p.240.
9 重有色金属材料加工手册编写组,重有色金属材料加工手册,(第四分册),冶金工业出版社,1980,p.19.
10 许其亮,未发表资料,1983.
No related articles found!