| 金属晶粒Euler指数与直径的相对等值规律 |
| 刘国权 |
| 北京钢铁学院 |
|
| EQUIVALENCE PRINCIPLE BETWEEN NORMALIZED EULER INDICES AND DIAMETER OF METAL GRAIN |
| LIU Guoquan (Beijing University of Iron and Steel Technology) |
引用本文:
刘国权. 金属晶粒Euler指数与直径的相对等值规律[J]. 金属学报, 1987, 23(1): 86-88.
.
EQUIVALENCE PRINCIPLE BETWEEN NORMALIZED EULER INDICES AND DIAMETER OF METAL GRAIN[J]. Acta Metall Sin, 1987, 23(1): 86-88.
1 Desch C.J Inst Met,1919;22:241 2 Williams W M,Smith C S.Trans AIME 1952;194:755 3 Okazaki K,Conrad H.Trans Jpn Inst Met,1972;13:198 4 Rhines F N,Patterson B R.Metall Trans 1982;13A:985 5 Liu G Q(刘国权).Ph.D Dissertation.Univ.of Florida,Gainesville FL,1984 6 DeHoff R T,Liu G Q(刘国权).Metall Trans,1985;16A:2007. 7 Smith C S.In:Metal Interfaces,Cleveland:ASM,1952,65E |
|