| 定向凝固合金DZ-38G的滑移形变与断裂 |
| 尹万全;高薇;朱桂秋;胡壮麒 |
| 中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所 |
|
| SLIP DEFORMATION AND FRACTURE OF DIRECTIONALLY SOLIDIFIED DZ-38G SUPERALLOY |
| YIN Wanquan; GAO Wei; ZHU Guiqiu; HU Zhuangqi (Institute of Metal Research; Academia Sinica; Shenyang) (Manuscript received 3 December. 1985; revised manuscript 11 June; 1986) |
引用本文:
尹万全;高薇;朱桂秋;胡壮麒. 定向凝固合金DZ-38G的滑移形变与断裂[J]. 金属学报, 1987, 23(3): 243-316.
,
,
,
.
SLIP DEFORMATION AND FRACTURE OF DIRECTIONALLY SOLIDIFIED DZ-38G SUPERALLOY[J]. Acta Metall Sin, 1987, 23(3): 243-316.
1 徐永波,穆在勤,刘民治,杨淑华.科学通报,1981:26:1356 2 Yin Wanquan (尹万全), Su Huihe (苏会和), Tong Yingjie (佟英傑), Liu Minzhi (刘民治). Int. Syrup. on Microstructure and Mechani cal Behaviour of Materials, Oct. 1985, Xi'an, China, Sponsored by Xi'an Jiaotong University, 1985; 29 3 林栋梁,黄颂惠.材料科学与工程,1985;(1) :4 |
|