| 轻轨钢腐蚀锈层分析及其对耐蚀性影响 |
| 魏翔云;李有柯 |
| 中国科学院金属腐蚀与防护研究所;中国科学院金属腐蚀与防护研究所 |
|
| STRUCTURE OF CORROSION RUST LAYERS ON SEVERAL LIRHT RAILWAY STEELS AND THEIR EFFECTS ON CORROSION RESISTANCE |
| WEI Xiangyun; LI Youke (Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang) (Manuscript received 29 January; 1986; revised manuscript 31 July; 1986) |
引用本文:
魏翔云;李有柯. 轻轨钢腐蚀锈层分析及其对耐蚀性影响[J]. 金属学报, 1987, 23(3): 246-249.
,
.
STRUCTURE OF CORROSION RUST LAYERS ON SEVERAL LIRHT RAILWAY STEELS AND THEIR EFFECTS ON CORROSION RESISTANCE[J]. Acta Metall Sin, 1987, 23(3): 246-249.
1 北京钢铁学院金属腐蚀教研组.金属腐蚀原理(二),1979 2 杨文治.电化学基础,北京大学出版社,1982 3 岡田秀弥,细井祜三,汤川憲一,内藤浩光.鉄鋼,1969;55(5) ;355-365岡田秀弥.防食技术,1971;20(4) :178-191O |
|