金属学报  1987, Vol. 23 Issue (4): 339-340    
  论文 本期目录 | 过刊浏览 |
中碳钢缺口端部疲劳裂纹萌生的临界应力
林吉忠;刘淑华;吴玉树;李一
铁道科学研究院;铁道科学研究院;铁道科学研究院;铁道科学研究院
THE CRITICAL STRESS OF FATIGUE CRACK INITIATION FOR MEDIUM CARBON STEEL
by LIN Jizhong; LIU Shuhua; WU Yushu; LI Yi (China Academy of Railway Sciences) (Manuscript received 22 April; 1986; revised manuscript 25 August; 1986)
引用本文:

林吉忠;刘淑华;吴玉树;李一. 中碳钢缺口端部疲劳裂纹萌生的临界应力[J]. 金属学报, 1987, 23(4): 339-340.
, , , . THE CRITICAL STRESS OF FATIGUE CRACK INITIATION FOR MEDIUM CARBON STEEL[J]. Acta Metall Sin, 1987, 23(4): 339-340.

全文: PDF(118 KB)  
摘要: <正> 本文选用四种中碳钢,其含碳量及机械性能列于表1.表1中的字母Ⅰ,Ⅱ分別代表一次正火及二次正火加回火的热处理工艺.
Abstract:Notch fracture machanics was used to investigate the fatigue crack initiation from the notch tip for medium carbon steels (0.4-0.6 wt-%C). The relationships between the maximum stress range at the notch root, △σ_(max), and the number of cycles before fatigue crack initiation, N_i, have been determined. Furthermore, the threshold stress of fatigue crack initiation, △σ_(max)th, as a function of C content or of yield strength of the steel has been proposed.