| 高炉气体力学电模拟研究 |
| 黎英豪 |
| 北京钢铁学院 |
|
| ELECTRICAL ANALOG OF PNEUMATIC PHENOMINA IN BLAST FURNACE |
| by LI Yinghao(Beijing University of Iron and Steel Technology)(Manuscript received 16 September; 1985; revised manuscript 24 November; 1986) |
引用本文:
黎英豪. 高炉气体力学电模拟研究[J]. 金属学报, 1987, 23(5): 447-451.
.
ELECTRICAL ANALOG OF PNEUMATIC PHENOMINA IN BLAST FURNACE[J]. Acta Metall Sin, 1987, 23(5): 447-451.
1 古金玛赫.电模型,科学出版社,1958:100 2 北京钢铁学院.冶金传输原理,北京钢铁学院教材科出版,1981:28 3 清华大学.流体力学基础,机械工业出版社,1982:40 4 杨永宜.炼铁,1983;1:9O |
|