| Cu-Al-Zn-Mn-Ni合金马氏体形态和晶体结构对伪弹性的影响 |
| 杨建华;刘彩虹;赵连城;雷廷权 |
| 哈尔滨工业大学;哈尔滨工业大学;哈尔滨工业大学;哈尔滨工业大学 |
|
| INFLUENCE OF MARTENSITE MORPHOLOGY AND CRYSTAL STRUCTURE ON THE PSEUDOELASTICITY IN A Cu-Al-Zn-Mn-Ni ALLOY |
| by YANG Jianhua; LIU Caihong; ZHAO Liancheng; LEI Tingquan (Harbin Institute of Technology) (Manuscript received 25 october; 1985; revised manuscript 15 July; 1986) |
引用本文:
杨建华;刘彩虹;赵连城;雷廷权. Cu-Al-Zn-Mn-Ni合金马氏体形态和晶体结构对伪弹性的影响[J]. 金属学报, 1987, 23(6): 470-476.
,
,
,
.
INFLUENCE OF MARTENSITE MORPHOLOGY AND CRYSTAL STRUCTURE ON THE PSEUDOELASTICITY IN A Cu-Al-Zn-Mn-Ni ALLOY[J]. Acta Metall Sin, 1987, 23(6): 470-476.
1 Abu-Arab A, Chandrasekaran M, Ahlers M. Scr Metall, 1984; 18: 709 2 赵连城,杨建华,刘乃华,雷廷权.稀有金属,1986,5:281 3 Yang J H, Zhao L C, Zhang C S, Lei T C. Scr Metall, 1987; 21(3) 4 赵连城,杨建华,刘乃华,张春生,雷廷权,顾华,何永枢.金属学报,1987;23A380: 5 Delaey L, Krishnan R V, Tas H, Warlimont H. J Mater Sci, 1974; 9: 1521 6 Van Humbeeck J. Janssen J, Mwamba-Ngoie, Delaey L. Scr Metall, 1984; 18: 893 7 Delaey L, Suzuki T, Van Humbeeck J. Scr Metall, 1984; 18: 899 |
|