| 4Cr5MoVSi(H11)钢的内氧化型渗碳层组织的研究 |
| 郝士明;孙荣耀 |
| 东北工学院;东北工学院 |
|
| MICROSTRUCTURE OF SURFACE LAYER FOR STEEL 4Cr5MoVSi AFTER CARBIDE DISPERSION CARBURIZING |
| by HAO Shiming; SUN Rongyao (Northeast University of Technology; Shenyang) (Manuscript received 26 June; 1986; revised manuscript 16 February; 1987) |
引用本文:
郝士明;孙荣耀. 4Cr5MoVSi(H11)钢的内氧化型渗碳层组织的研究[J]. 金属学报, 1987, 23(6): 588-591.
,
.
MICROSTRUCTURE OF SURFACE LAYER FOR STEEL 4Cr5MoVSi AFTER CARBIDE DISPERSION CARBURIZING[J]. Acta Metall Sin, 1987, 23(6): 588-591.
1 Murphy R J, Grant N J. Trans ASM, 1967;60(1) :29 2 千葉昂,齋藤卓,高山武盛,郝士明,西沢泰二.铁钢,1981;67(2) :A61 3 郝士明,高山武盛,西沢泰二.日本金属学会读,1981;45:1195 4 郝土明.东北工学院学报,1983;36(3) :21 5 Uhrenius B. Hardenability Concepts with Applications to Steel, Doane, Kirkaldy eds., AIME, 1978 6 Hillert M,赖和怡,刘国勋译.合金扩散和热力学,北京:冶金工业出版社,1984* |
|