| 晶体生长的初始成分过渡区 |
| 李言祥;柳百成 |
| 清华大学机械工程系;清华大学机械工程系;教授 |
|
| INITIAL COMPOSITION TRANSIENT DURING CRYSTAL GROWTH |
| LI Yanxiang;LIU Baicheng Department of Mechanical Engineering; Tsinghua University; Beijing |
引用本文:
李言祥;柳百成. 晶体生长的初始成分过渡区[J]. 金属学报, 1988, 24(1): 82-86.
,
.
INITIAL COMPOSITION TRANSIENT DURING CRYSTAL GROWTH[J]. Acta Metall Sin, 1988, 24(1): 82-86.
1 Tiller W A, Jackson K A, Rutter J W, Chalmers B. Acta Metall, 1953; 1: 428 2 闵乃本.晶体生长的物理基础,上海科学技术出版社,1982:58 3 Pohl R G. J Appl Phys, 1954; 23: 1170 4 Flemings M C. Solidification Processing, New York: McGraw-Hill, 1974: 4 |
|