| 含氧化钛高炉型渣表面张力的测定 |
| 杨祖磐;吴铿;黄振奇 |
| 沈阳东北工学院冶金物化教研室;教授;东北工学院;北京钢铁学院博士研究生;东北工学院 |
|
| SURFACE TENSION OF BLAST FURNACE TYPE SLAGS CONTAINING TITANIUM OXIDES |
| YANG Zupan Professor;Laboratory of Metallurgical Physical Chemistry;Northeast University of Technology;Shenyang;WU Keng;HUANG Zhenqi Northeast University of Technology; Shenyang |
引用本文:
杨祖磐;吴铿;黄振奇. 含氧化钛高炉型渣表面张力的测定[J]. 金属学报, 1988, 24(2): 210-213.
,
,
.
SURFACE TENSION OF BLAST FURNACE TYPE SLAGS CONTAINING TITANIUM OXIDES[J]. Acta Metall Sin, 1988, 24(2): 210-213.
1 Sohn H Y, Wadsworth M E. Rate Processes of Extractive Metallurgy, New York: Plenum Press, 1979: 354 2 杨世泽,刘清才.钢铁钒钛,1985;(1) :11 3 徐鸿飞,潘竞业,石世雄.钢铁钒钛,1984;(2) :26 4 工文忠.钢铁钒钛,1984;(2) :47 5 朱元凯,毛裕文,郭昭信,王功厚,董亚隆.钢铁钒钛,1983;(1) :14 6 王喜庆.四川冶金,1982;3 7 White D W G.Trans ASM,1962;55:757 8 溶钢溶滓部会报告.溶铁.溶滓物性值便览,1971:137 9 Bathforth F, Adams JC. An Attempt to test the Theories of Capillary Action, London: Cam bridge University Press. 1883: BII 1--26 10 Gallois B. Lupis C H P. Metall Trans, 1981; 12B: 679 11 小竹无二雄.实验化学讲座,9无机物合成精制,1956& |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|