| 母相晶粒度和有序度对含硼Cu-Zn-Al合金形状记忆效应的影响 |
| 吴建新;江伯鸿;徐祖耀 |
| 上海交通大学;上海交通大学;上海交通大学 |
|
| INFLUENCE OF GRAIN SIZE AND ORDERING DEGREE OF PARENT PHASE ON SHAPE MEMORY EFFECT IN A CuZnAl ALLOY CONTAINING BORON |
| WU Jianxin;JIANG Bohong;Hsu T. Y. XU Zuyao Shanghai Jiao Tong University |
引用本文:
吴建新;江伯鸿;徐祖耀. 母相晶粒度和有序度对含硼Cu-Zn-Al合金形状记忆效应的影响[J]. 金属学报, 1989, 25(3): 17-22.
,
,
.
INFLUENCE OF GRAIN SIZE AND ORDERING DEGREE OF PARENT PHASE ON SHAPE MEMORY EFFECT IN A CuZnAl ALLOY CONTAINING BORON[J]. Acta Metall Sin, 1989, 25(3): 17-22.
1 Perkins J. Mater Sci Eng, 1981; 51: 181 2 Qi X (漆璿), Jiang B H (江伯鸿), Hsu T Y (Xu Zuyao) (徐祖耀). Mater Sci Eng, 1987; 93: 205 3 Miyazaki S, Otsuka K, Sakamoto H, Shimizu K. Trans Jpn Inst Met, 1981; 4: 244 4 Lee J S. Wayman C M. Metallography, 1986; 19: 401 5 Adnyana D N. Metallography, 1985; 18: 187 6 Melton K N, Mercier O. In: Haason P, Gerold V, Kostorz G eds., Strength of Metals and Alloys, Vol. Ⅱ, Proc 5th Int Conf, Aachen, FRG. Aug. 27--31, 1979, Pergamon Press, 1980: 1243 7 Sugimoto K. J Phys, (Paris), Colloque C4, Supplement au №12, 1982; 43: C4--761 8 Wu J K (吴建新), Jiang B H (江伯鸿), Hsu T Y (Xu Zuyao) (徐祖耀). Acta Metall., 1988; 6: 1521 9 Weibel E R. Morphometry of the Humanlung Berlin: Springer-Verlag, 1963 10 Iain L M. Principle of Mechanical Metallurgy, London: Arnold, 1981: 185 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|