| 非晶态合金Fe_(71)Ni_(10)B_(13)Si_4C_2磁各向异性的Mssbauer谱研究 |
| 徐祖雄;马如璋;韩永柱 |
| 北京科技大学;北京科技大学;北京冶金研究所 |
|
| MSSBAUER STUDY ON MAGNETIC ANISOTROPY OF AMORPHOUS ALLOY Fe_(71)Ni_(10)B_(13)Si_4C_2 |
| XU Zuxiong;MA Ruzhang;HAN Yongzhu University of Science and Technology Beijing Beijing Institute of Metallurgy |
引用本文:
徐祖雄;马如璋;韩永柱. 非晶态合金Fe_(71)Ni_(10)B_(13)Si_4C_2磁各向异性的Mssbauer谱研究[J]. 金属学报, 1989, 25(3): 143-145.
,
,
.
MSSBAUER STUDY ON MAGNETIC ANISOTROPY OF AMORPHOUS ALLOY Fe_(71)Ni_(10)B_(13)Si_4C_2[J]. Acta Metall Sin, 1989, 25(3): 143-145.
1 Ok H N, Morrish A H. Phys Rev B, 1981; 23: 2257 2 Gonser U, Ackermann M, Wagner H G. J Magn Magn Mater. 1983, 31--34: 1605 3 Xu Zuxiong (徐祖雄), Ma Ruzhang (马如璋), Ping Jueyun (平爵云). Sci Sin. A, 1985; 28: 215 4 Schaafsma A S, Snijiders H, van der Woude F, Drijiver J W, Radelaar S. Phys Rev B, 1979; 20: 4423 |
|