金属学报  1989, Vol. 25 Issue (5): 15-18    
  论文 本期目录 | 过刊浏览 |
Ti-Ni-Fe合金的无公度相变和公度相变
饶建锡;马如璋;何豫生
海军工程学院;北京科技大学;清华大学
INCOMMENSURATE AND COMMENSURATE PHASE TRANSITIONS IN Ti-Ni-Fe ALLOY
RAO Jianxi;MA Ruzhang;HE Yusheng Naval Academy of Engineering Wuhan University of Scicnce and Technology Beijing Tsinghua University; Beijing MA Ruzhang;professor;Faculty of Metal Fhysics;University of Science and Technology Beijing; 100083 Beijing
引用本文:

饶建锡;马如璋;何豫生. Ti-Ni-Fe合金的无公度相变和公度相变[J]. 金属学报, 1989, 25(5): 15-18.
, , . INCOMMENSURATE AND COMMENSURATE PHASE TRANSITIONS IN Ti-Ni-Fe ALLOY[J]. Acta Metall Sin, 1989, 25(5): 15-18.

全文: PDF(372 KB)  
摘要: 本文通过对Ti-Ni-Fe合金同时进行超声测量与电阻测量,证实降温过程的第一个声速谷主要是由驱动公度(R)相变的软模引起的,第二个声速谷归于驱动马氏体(M)相变的软模。确定了这种合金的公度相变的起始点R_s和结束点R_f。
关键词 : 无公度(Ⅰ)相变,  公度相变,  Ti-Ni-Fe合金    
Abstract:Measurements by using the ultrasonic technique together for electricresistance verified that the first sound velocity valley on cooling is mainly due tothe soft-mode of driving the commensurate phase transition, and the second onedue to the soft-mode of driving the martensitic transformation. The starting point,R_s, and finishing point, R_f, of the commensurate phase transition of the alloyhave been determined.
Key words: incommensurate phase transition    commensurate phase transition    Ti-Ni-Fe alloy
收稿日期: 1989-05-18     
1 Hwang C M, Meichle M, Salamon M B, Wayman C M. Philos Mag, 1983; A47: 9, 31, 177
2 Nishida M, Wayman C M, Honma T. Metallography, 1986; 19: 99
3 王大志,朱斌,周贵恩,俞文海.物理学报,1987; 36: 1004
4 Ling H C, Kaplow R. Metall Trans, 1980; 11A: 77
5 饶建锡.北京科技大学博士论文,1988
6 饶建锡,马如璋.北京钢铁学院学报(专刊),1987;(1) :63
7 Salamon M B, Meichle M E, Wayman C M. Phys Rev B, 1985; 31: 7306
8 Mo C M, Chen B P, Chen L, Qin Y, Gao Y M, Shen H, Guo J F. Proc Int Symp on Shape Memory Alloys, Beijing: China Academic, 1986: 159Z
No related articles found!