| Cu-Zn-Al-Mn合金的贝氏体中脊和台阶 |
| 韩明;陈复民;陈金铭;陈玉如;刘文西 |
| 天津大学;浙江大学材料科学与工程系;天津大学材料科学与工程系;教授;天津(300072);天津大学;天津大学;天津大学 |
|
| MIDRIB AND LEDGE OF BAINITE IN A Cu-Zn-Al-Mn ALLOY |
| HAN Ming;CHEN Fumin;CHEN Jinming;CHEN Yuru;LIU Wenxi Tianjin University professor;Department of Material Science and Engineering;Tianjin University; Tianjin 300072 |
引用本文:
韩明;陈复民;陈金铭;陈玉如;刘文西. Cu-Zn-Al-Mn合金的贝氏体中脊和台阶[J]. 金属学报, 1990, 26(2): 5-9.
,
,
,
,
.
MIDRIB AND LEDGE OF BAINITE IN A Cu-Zn-Al-Mn ALLOY[J]. Acta Metall Sin, 1990, 26(2): 5-9.
1 陈树川,张骥华,张寿柏,徐祖耀.金属学报,1986;22:A379 2 刘文西,邹美运,马福本.金属学报,1981;17:137 3 Okamoto H, Oka M. Metall Trans, 1986; 17A: 1113 4 Chattopadhyay K, Aaronson H I. Acta Metall, 1986; 34: 695 5 Cornelis I, Wayman C M. Scr Metall, 1973; 7: 579 6 Lorimer G W, Cliff G, Aaronson H I, Kinsman K R. Scr Metall, 1975; 9: 27 |
|