金属学报  1990, Vol. 26 Issue (2): 5-9    
  论文 本期目录 | 过刊浏览 |
Cu-Zn-Al-Mn合金的贝氏体中脊和台阶
韩明;陈复民;陈金铭;陈玉如;刘文西
天津大学;浙江大学材料科学与工程系;天津大学材料科学与工程系;教授;天津(300072);天津大学;天津大学;天津大学
MIDRIB AND LEDGE OF BAINITE IN A Cu-Zn-Al-Mn ALLOY
HAN Ming;CHEN Fumin;CHEN Jinming;CHEN Yuru;LIU Wenxi Tianjin University professor;Department of Material Science and Engineering;Tianjin University; Tianjin 300072
引用本文:

韩明;陈复民;陈金铭;陈玉如;刘文西. Cu-Zn-Al-Mn合金的贝氏体中脊和台阶[J]. 金属学报, 1990, 26(2): 5-9.
, , , , . MIDRIB AND LEDGE OF BAINITE IN A Cu-Zn-Al-Mn ALLOY[J]. Acta Metall Sin, 1990, 26(2): 5-9.

全文: PDF(1842 KB)  
摘要: 用透射电镜详细地研究了Cu-Zn-Al-Mn合金的贝氏体相变。观察结果表明:该合金中贝氏体在形成初期已存在层错。同时观察到贝氏体中脊,贝氏体内部的层错面能够连续地通过中脊。在贝氏体宽面及端部存在长大台阶,台阶的宽面和窄面分别平行于贝氏体层错面和惯习面,其晶面指数均属{110}_(B2)晶面族,长大台阶的推进方向平行于层错面。由此推测,Cu-Zn-Al-Mn合金贝氏体在相变初期首先以切变方式形成,而其长大过程是由其层错面的扩展所控制。
关键词 Cu-Zn-Al-Mn合金贝氏体中脊长大台阶    
Abstract:The bainitic transformation in a Cu-Zn-Al-Mn alloy has been examin-ed with TEM. The results show that the stacking faults and also the bainitic mi-drib are found at the beginning of bainite formation in the alloy. The stack-ing fault planes can pass continuously through the midrib in bainite. The growthledges occur at the broad faces and rims of bainite. The broad and narrow faces ofthe ledges are parallel to the fault plane and habit plane respectively. Both theirMiller indices are {110}_(B_2). The moving direction of ledges is parallel to the faultplane. It may be deduced that bainites in a Cu-Zn-Al-Mn alloy are initially form-ed by shear and the process of growth are governed by propagation of fault planes.
Key wordsCu-Zn-Al-Mn alloy    bainitic midrib    growth ledge
收稿日期: 1990-02-18     
基金资助:国家自然科学基金资助项目
1 陈树川,张骥华,张寿柏,徐祖耀.金属学报,1986;22:A379
2 刘文西,邹美运,马福本.金属学报,1981;17:137
3 Okamoto H, Oka M. Metall Trans, 1986; 17A: 1113
4 Chattopadhyay K, Aaronson H I. Acta Metall, 1986; 34: 695
5 Cornelis I, Wayman C M. Scr Metall, 1973; 7: 579
6 Lorimer G W, Cliff G, Aaronson H I, Kinsman K R. Scr Metall, 1975; 9: 27
No related articles found!