| Ti-13at.-%Ni-37at.-%Pd记忆合金预形变与高温形状记忆效应 |
| 李永森;金永柏;于荣海 |
| 中国科学院金属研究所;副研究员;沈阳(110015);中国科学院金属研究所;中国科学院金属研究所 |
|
| HIGH TEMPERATURE SHAPE MEMORY EFFECT OF PRE-DEFORMATION FOR Ti_(50)Ni_(13)Pd_(37) ALLOY |
| LI Yongsen;JIN Yongbai;YU Ronghai Institute of Metal Research; Academia Sinica; Shenyang associate professor;Institute of Metal Research;Academia Sinica; Shenyang 110015 |
引用本文:
李永森;金永柏;于荣海. Ti-13at.-%Ni-37at.-%Pd记忆合金预形变与高温形状记忆效应[J]. 金属学报, 1990, 26(2): 37-40.
,
,
.
HIGH TEMPERATURE SHAPE MEMORY EFFECT OF PRE-DEFORMATION FOR Ti_(50)Ni_(13)Pd_(37) ALLOY[J]. Acta Metall Sin, 1990, 26(2): 37-40.