| PbS和PbO反应动力学及其机理 |
| 李诚;刘纯鹏 |
| 北京有色冶金设计研究总院冶炼一室;北京(100038);昆明工学院 |
|
| KINETICS OF REACTION BETWEEN PbS AND PbO |
| LI Cheng;LIU Chunpeng Beijing Central Design and Research Institute for Non-Ferrous Metallurgical Industry Kunming Institute of Technology Metallurgical Department No.1;Beijing Central Design and Research Institute for Non-Ferrous Metallurgical Industry; Beijing 100038 |
引用本文:
李诚;刘纯鹏. PbS和PbO反应动力学及其机理[J]. 金属学报, 1990, 26(2): 83-87.
,
.
KINETICS OF REACTION BETWEEN PbS AND PbO[J]. Acta Metall Sin, 1990, 26(2): 83-87.