| Au-Cu-Si三元系液相限 |
| 刘淑祺;易涛 |
| 副教授;北京(100871);北京大学化学系;北京大学化学系 |
|
| LIQUIDUS OF Au-Cu-Si SYSTEM |
| LIU Shuqi;YI Tao Department of Chemistry; Peking University; Beijing |
引用本文:
刘淑祺;易涛. Au-Cu-Si三元系液相限[J]. 金属学报, 1990, 26(4): 153-154.
,
.
LIQUIDUS OF Au-Cu-Si SYSTEM[J]. Acta Metall Sin, 1990, 26(4): 153-154.
1 Massalski T B. Binary Alloy Phase Diagrams, Metals Park, Ohio: ASM, 1986: 254, 313, 960 2 刘淑祺,孙文庆.金属学报,1988;24:B376 |
|