| 粗晶纯Al多晶材料的循环形变——Ⅰ.滑移特征 |
| 夏月波;王中光 |
| 中国科学院金属研究所;材料疲劳与失效分析国家重点实验室副研究员;沈阳110015;中国科学院金属研究所;材料疲劳与失效分析国家重点实验室 |
|
| CYCLIC DEFORMATION OF COARSE GRAINED POLYCRYSTALLINE PURE Al Ⅰ. SLIP CHARACTERISTICS |
| XIA Yuebo;WANG Zhongguang State Key Laboratory for Fatigue and Failure of Materials; Institute of Metal Research; Academia Sinica; Shenyang |
引用本文:
夏月波;王中光. 粗晶纯Al多晶材料的循环形变——Ⅰ.滑移特征[J]. 金属学报, 1992, 28(2): 3-8.
,
.
CYCLIC DEFORMATION OF COARSE GRAINED POLYCRYSTALLINE PURE Al Ⅰ. SLIP CHARACTERISTICS[J]. Acta Metall Sin, 1992, 28(2): 3-8.
| 1 Lim L C, Raj R. Acta Metall, 1985; 33: 2205
2 Lim L C, Raj R. Acta Metall, 1984; 32: 1177
3 Okada T, Onaka S, Hashimoto S, Miura S. Scr Metall, 1989; 23: 49
4 Basinski Z S, Basinski S J. Acta Metall, 1985; 33: 1307
5 Jin N Y. Acta Metall, 1989; 37: 2055
6 Wang Zhongguang, Hu Tianbao, Xia Yuebo, Yang Qibin. Chin J Met Sci Technol, 1986; 2: 367
7 Liu Wei, Wang Zhongguang, Xia Yuebo. Chin J Met Sci Technol, 1989; 5: 123
8 Liu Wei, Wang Zhongguang, Xia Yuebo. Phys Status Solidi(a), 1989; 114: 177
9 林栋梁,吴建生.金属学报,1988;24:A76 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|