| 粗晶纯Al多晶材料的循环形变——Ⅱ.断口形貌 |
| 夏月波;王中光 |
| 中国科学院金属研究所;材料疲劳与断裂国家重点实验室;中国科学院金属研究所;材料疲劳与断裂国家重点实验室 |
|
| CYCLIC DEFORMATION OF COARSE GRAINED POLYCRYSTALLINE PURE Al Ⅱ. FRACTURE SURFACE MORPHOLOGY |
| XIA Yuebo;WANG Zhongguang State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; Academia Sinica; Shenyang |
引用本文:
夏月波;王中光. 粗晶纯Al多晶材料的循环形变——Ⅱ.断口形貌[J]. 金属学报, 1992, 28(3): 21-26.
,
.
CYCLIC DEFORMATION OF COARSE GRAINED POLYCRYSTALLINE PURE Al Ⅱ. FRACTURE SURFACE MORPHOLOGY[J]. Acta Metall Sin, 1992, 28(3): 21-26.
1 曾祥华.中国科学院院刊,1986;1:121
2 夏月波,王中光,艾素华.金属学报,1982;18:606 3 Xia Y B, Wang Z G, Wang R H. Phys Status Solidi (a), 1990; 120: 125 4 夏月波,王中光.金属学报,1992;28(2) :A51 5 Gerberich W W, Jatavallabhula K. Acta Metall, 1983; 31: 241 6 Bucci R J, Paris P C, Herterzberg R W, Schmidt R A, Anderson A F. ASTM STP 513, 1972: 125 7 Hertzberg R W, Mills W J. ASTM STP 600, 1975: 220 8 Gell M, Leverant G R. Acta Metall, 1968; 16: 553 9 Feeney J A, McMillan J C, Wei R P. Metall Trans, 1970; 1: 429 10 Otsuka A, Mori K, Miyata T. Eng Fract Mech, 1975; 7: 429 11 Bechem C D, Meyn D A. ASTM STP 436, 1968: 59 12 Gell M, Leverant G R. Trans Am Inst Min Metall Pet Eng, 1968; 242: 1869 13 Phillips A, Kerlins V, Rawe R A, Whiteson B V. Electorn Fractography Handbook. Battelle, Metals and Ceramics Information Center, 19767 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|