| 高速钢中马氏体二次硬化的TEM研究 |
| 邱军;袁逸;陈景榕 |
| 北京科技大学;北京科技大学;北京科技大学材料系金相教研室;北京100083 |
|
| TEM STUDY OF SECONDARY HARDENING OF MARTENSITE IN HIGH SPEED STEEL |
| QIU Jun; YUAN Yi; CHEN Jingrong(University of Science and Technology Beijing) |
引用本文:
邱军;袁逸;陈景榕. 高速钢中马氏体二次硬化的TEM研究[J]. 金属学报, 1992, 28(7): 19-24.
,
,
.
TEM STUDY OF SECONDARY HARDENING OF MARTENSITE IN HIGH SPEED STEEL[J]. Acta Metall Sin, 1992, 28(7): 19-24.
1 Kuo Kehsin. J Iron Steel Inst, 1953; 174: 223 Kuo Kehsin. J Iron Steel Inst, 1953; 173: 363 2 Fischmeister H F, Karagoez S, Andren H O. Acta Metall, 1988; 36: 817 3 陈景榕,朱煜铎.金属科学与工艺,1986;5(1) :1 4 郭可信.X射线学及电子显微术的进展.上海:上海科学技术出版社,1966:36 5 Edington J W. Practical Electron Microscopy in Materials Science. Part Ⅱ, 1971:70 6 Jack K H. Nitriding, Heat Treatment. London: The Metals Society, 1973 7 E1 Rakayby A M, Mills B. Mater Sci Technol, 1986; 2: 175 8 Raynor D, Whiteman J A, Honeycombe R W K. J Iron Steel Inst, 1966; 204: 1114 |
|