Please wait a minute...
金属学报  1993, Vol. 29 Issue (9): 53-59    
  论文 本期目录 | 过刊浏览 |
无捕收剂浮选时硫化矿物表面的疏水-亲水平衡关系
孙水裕;王淀佐;李柏淡
中南工业大学;中南工业大学;中南工业大学
HYDROPHOBICITY-HYDROPHILICITY BALANCE RELATIONSHIPS FOR COLLECTORLESS FLOTATION OF SULPHIDE MINERALS
SUN Shuiyu;WANG Dianzuo;LI Bodan Department of Mineral Engineering; Central South University of Technology; Changsha
引用本文:

孙水裕;王淀佐;李柏淡. 无捕收剂浮选时硫化矿物表面的疏水-亲水平衡关系[J]. 金属学报, 1993, 29(9): 53-59.
, , . HYDROPHOBICITY-HYDROPHILICITY BALANCE RELATIONSHIPS FOR COLLECTORLESS FLOTATION OF SULPHIDE MINERALS[J]. Acta Metall Sin, 1993, 29(9): 53-59.

全文: PDF(600 KB)  
摘要: 通过硫化矿物表面中性硫(S~o)的溶剂提取-化学分析、矿浆电位测定和浮选试验,建立了自诱导浮选和硫化钠诱导浮选的疏水-亲水平衡关系,分别用[S~o]/[OH~-]和[S~o]/[OH~-]+[HS~-])表示S~o的生成量[S~o]受矿浆电位调控研究结果表明,pH值相同时,[S~o]值越大,矿物表面疏水性高,浮选行为好pH值高,[OH~-]值高,矿物表面亲水性大,浮选需要的[S~o]多;反之亦然同一pH值下,硫化钠诱导浮选所需[S~o]较自诱导浮选高
关键词 : 疏水-亲水平衡,  自诱导浮选,  硫化钠诱导浮选    
Abstract:Hydrophobicity-hydrophilicity balance relationships for collectorlessflotation, including self-induced and Na_2S-induced flotation, have been established, throughsolvent extraction-chemical analyses of neutral sulphur (S~0) from sulphide mineral surfaces,measurements of pulp potential and flotation tests. They may be indicated as [S~0]/[OH~-]and[S~0]/([OH~-]+[HS~-]) respectively. The neutral sulphur extracted was considered to be re-sponsible for the hydrophobicity, and the amount of which was controlled by pulp potential.The critical value of neutral sulphur amount was proposed as a new concept, and was used toindicate the hydrophobic degree and flotation behaviour. The hydrophilicity was attributed toOH~- ion for self-induced flotation and both OH~- and HS~- ions for Na_2S-inducedflotation. At a given pH value, hydrophobicity and floatability increase with the amount ofneutral sulphur extracted. At different pH values, the higher pH results in the strongerhydrophilicity, and hence hydrophobicity and flotation require more amount of S~0. The lowerpH values are in correspondence with smaller amount of S~0. The critical value of amount ofS~0 to Na_2S-induced flotation is higher than that to self induced flotation because of thehydrophilicity of HS~- ions.
Key words: Hydrophobicity-hydrophilicity balance    Na_2S-induced flotation    self-induced flotation
收稿日期: 1993-09-18     
基金资助:国家自然科学基金
1 Sutherland K L, Wark I W. Principles of Flotation. Melbourne: Australian Inst Min Metal, 1955: 119
2 Barsky G. Trans Am Inst Min Metall Eng, 1934; 112: 236
3 Trahar W J. In: Jones M H, Woodcook J T eds., Principles of Mineral Flotation, Proc Austrian IMM, Parkville, Australia: Australian Inst Min Metal, 1984: 117
4 Buckley A N, Walker G W. In: Forssberg E ed, Proc 16th Int Miner Processing Congress, Stokholm: The Swedish IMM, 1988: 589
5 Walker G W, Richardson P E, Buckley A N. Int J Miner Process, 1989; 25: 155
6 孙水裕,王淀佐,李柏淡.中南矿冶学院学报(选矿专辑),1991;22(3) :43
7 孙水裕,王淀佐,李柏淡.中南矿冶学院学报,1993;24(2) :181
8 孙水裕,王淀佐,李柏淡.有色金属(季刊),1993;45(2) :32
9 孙水裕,王淀佐,李柏淡.有色金属(季刊),1992;44(2) :17;
No related articles found!