无捕收剂浮选时硫化矿物表面的疏水-亲水平衡关系 |
孙水裕;王淀佐;李柏淡 |
中南工业大学;中南工业大学;中南工业大学 |
|
HYDROPHOBICITY-HYDROPHILICITY BALANCE RELATIONSHIPS FOR COLLECTORLESS FLOTATION OF SULPHIDE MINERALS |
SUN Shuiyu;WANG Dianzuo;LI Bodan Department of Mineral Engineering; Central South University of Technology; Changsha |
引用本文:
孙水裕;王淀佐;李柏淡. 无捕收剂浮选时硫化矿物表面的疏水-亲水平衡关系[J]. 金属学报, 1993, 29(9): 53-59.
,
,
.
HYDROPHOBICITY-HYDROPHILICITY BALANCE RELATIONSHIPS FOR COLLECTORLESS FLOTATION OF SULPHIDE MINERALS[J]. Acta Metall Sin, 1993, 29(9): 53-59.
1 Sutherland K L, Wark I W. Principles of Flotation. Melbourne: Australian Inst Min Metal, 1955: 119 2 Barsky G. Trans Am Inst Min Metall Eng, 1934; 112: 236 3 Trahar W J. In: Jones M H, Woodcook J T eds., Principles of Mineral Flotation, Proc Austrian IMM, Parkville, Australia: Australian Inst Min Metal, 1984: 117 4 Buckley A N, Walker G W. In: Forssberg E ed, Proc 16th Int Miner Processing Congress, Stokholm: The Swedish IMM, 1988: 589 5 Walker G W, Richardson P E, Buckley A N. Int J Miner Process, 1989; 25: 155 6 孙水裕,王淀佐,李柏淡.中南矿冶学院学报(选矿专辑),1991;22(3) :43 7 孙水裕,王淀佐,李柏淡.中南矿冶学院学报,1993;24(2) :181 8 孙水裕,王淀佐,李柏淡.有色金属(季刊),1993;45(2) :32 9 孙水裕,王淀佐,李柏淡.有色金属(季刊),1992;44(2) :17; |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|