| 双滑移取向Cu单晶的循环形变行为──Ⅱ.滑移带和形变带 |
| 宫波;王中光;张轶伟;李广义;张天宜 |
| 中国科学院金属研究所材料疲劳与断裂国家重点实验室 |
|
| CYCLIC DEFORMATION BEHAVIOUR OF Cu SINGLE CRYSTALS ORIENTED FORDOUBLE SLIP Ⅱ. Persistent Slip Bands and Deformation Bands |
| GONG Bo; WANG Zhongguang; ZHANG Yiwei; LI Guangyi; ZHANG Tianyi(State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Re-search; Chinese Academy of Sctences; Shenyang)(Manuscript received 16 March; 1994) |
引用本文:
宫波;王中光;张轶伟;李广义;张天宜. 双滑移取向Cu单晶的循环形变行为──Ⅱ.滑移带和形变带[J]. 金属学报, 1994, 30(10): 439-447.
,
,
,
,
.
CYCLIC DEFORMATION BEHAVIOUR OF Cu SINGLE CRYSTALS ORIENTED FORDOUBLE SLIP Ⅱ. Persistent Slip Bands and Deformation Bands[J]. Acta Metall Sin, 1994, 30(10): 439-447.
| 1LairdC,FinneyJM,Kuhlmann-WilsdorfD.MaterSciEng,1981;50:1272宫波,王中光,张轶伟,李广义,张天宜.金属学报,1994,30:4313MaBT,LairdC.ActaMetall,1989;37:3254WinterAT.PhilosMag,1974;29:7195CahnRW.JInstMet,1950-1951;79:1296HoneycombeRKW.JInstMet,1951-1952;80:457CalnanEA.ActaCrystall,1952;5:5578GostelowCR.MetSciJ,1971;5:1779MughrabiH.MaterSciEng,1978;33:20710SaletoreM,TaggartRMaterSciEng,1978:36:259 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|