| 不同晶粒尺寸Ni-P合金纳米晶体的界面过剩体积研究 |
| 隋曼龄;卢柯 |
| 东北大学;中国科学院国际材料物理中心;中国科学院金属研究所快速凝固非平衡合金国家开放实验室 |
|
| INTERFACIAL EXCESS VOLUME IN NANOCRYSTALLINE Ni-P ALLOYS WITH DIFFERENT GRAIN SIZES |
| SUI Manling (Northeastern University; International Centre for Materials Physics;Chinese Academy of Sciences; Shenyang);LU Ke (Institute of Meial Research; Chinese Academy of Sciences; Shenyang) |
引用本文:
隋曼龄;卢柯. 不同晶粒尺寸Ni-P合金纳米晶体的界面过剩体积研究[J]. 金属学报, 1994, 30(15): 121-125.
,
.
INTERFACIAL EXCESS VOLUME IN NANOCRYSTALLINE Ni-P ALLOYS WITH DIFFERENT GRAIN SIZES[J]. Acta Metall Sin, 1994, 30(15): 121-125.
| 1LuK,WangJT,WeiWD.JApplPhys,1991;69:5222LuK.WeiWD,WangJTSerMetall,1990;24:23l93SuiML,XiongLY,DengW,LuK,PatuS,HeYZ.JApplPhys,199l;69:44514SuiML,LuK,HeYZ.PhilosMag,1991;B63:9935MillsAP,WilsonRJ.PhysRev1982;A26:4906SeegerA.ApplPhys,1974;4:1837SchaeferH-E.PhysStatusSolidi,1987;(a)102:478SuiML,PatuS,HeYZ.ScrMetallMater,1991;25:15379DonnayJDH,OndikHM.CrystalDataDeterTables.NBS&JCPDS,197310LuK.LuckR,PredelB.ScrMetallMater.1992;28:387, |
|