Please wait a minute...
金属学报  1994, Vol. 30 Issue (16): 187-193    
  论文 本期目录 | 过刊浏览 |
短纤维增强复合材料的仿生模型──Ⅱ 弱结合界面的强度理论
赵晓鹏;田晓滨;周本濂;李世红
中国科学院金属研究所;中国科学院国际材料物理中心
A BIOMIMETIC MODEL OF SHORT FIBRE REINFORCED COMPOSITE MATERIALS──Ⅱ Strength Theory of Imperfect-Bonding Interface
ZHAO Xiaopeng(Institute of Metal Research;Chinese Academy of Sciences;Shenyang;International Center for Materials Physics;Chinese Academy of Sciences;Shenyang);TIAN Hiaobin(Institute of Metal Research;Chinese Academy of Sciences;Shenyang);ZHOU Benlian(Institute of Metal Research;Chinese Academy of Sciences;Shenyang;International Center for Materials Physics;Chinese Academy of Sciences; Shenyang);LI Shihong(Institute of Metal Research;Chinese Academy of Sciences;Shenyang)(Manuscript received 28 July 1993;in revised form 8 November 1993)
引用本文:

赵晓鹏;田晓滨;周本濂;李世红. 短纤维增强复合材料的仿生模型──Ⅱ 弱结合界面的强度理论[J]. 金属学报, 1994, 30(16): 187-193.
, , , . A BIOMIMETIC MODEL OF SHORT FIBRE REINFORCED COMPOSITE MATERIALS──Ⅱ Strength Theory of Imperfect-Bonding Interface[J]. Acta Metall Sin, 1994, 30(16): 187-193.

全文: PDF(384 KB)  
摘要: 根据哑铃状增强纤维的仿生分析,建立了弱结合界面模型和理想弹塑性基体增强复合材料强度唯象理论.证明哑铃状纤维增强效果优于平直纤维.理论预测与实验结果吻合较好.
关键词 : 短纤维复合材料,  仿生,  弱结合界面    
Abstract:According to the biomimetic research for fibres with enlarged ends,the model of imperfect-bonding interface and the strength theory of composite materials with perfect elastic-plastic matrix have been put forward.It has also been proved that the tensile strength of composite materials reinforced by fibres with enlarged-ends is higher than that by plain fibres.The theoretical and experimental results are in fairly good agreement.Correspondent:ZHAO Xiaopeng,(Institute of Metal Research,Chinese Academy of Sciences,Shenyang 110015)
Key words: biomimetic design    imperfect-bonding interface    short fibre reinforced composite
    
基金资助:国家自然科学基金
1田晓滨,赵晓鹏,周本濂.金属学报,1994;30:B1802FiliouC,GaliotisC,BatchelderDN.Composites,1992;23:283JeronimidisG,ParkyuAT.JComposMater,1988;26:4014VedulaM,PangbornRN,QueeneyRA.Composites,1988;19:555HeckerSS,CooperAR.JMater,1970;5:10116BroutmanLJ,KrockRH.ModernCompositeMaterials.London:Addison-Wesley,1967:25
[1] 赵晓鹏;周本濂;罗春荣;刘建伟. 短纤维增强复合材料的仿生模型──Ⅲ.脆性基体复合材料中哑铃状纤维的强化作用[J]. 金属学报, 1996, 32(4): 438-442.
[2] 田晓滨;赵晓鹏;周本濂. 短纤维增强复合材料的仿生模型──Ⅰ 哑铃状短纤维增强复合材料的应力分析[J]. 金属学报, 1994, 30(16): 180-186.