Please wait a minute...
金属学报  1994, Vol. 30 Issue (9): 404-408    
  论文 本期目录 | 过刊浏览 |
单向、双向记忆合金的相变热测定
谭树松;徐惠彬
中南工业大学;北京航空航天大学
CALORIMETRIC MEASUREMENTS FOR ONE WAY AND TWO WAY CuZnAl MEMORY ALLOYS
TAN Shusong(Central South University of Technology; Changsha)XU Huibin (Beijing University of Aeronautics and Astronautics) MULLER L(Technische Universitat Berlin; Germany)(Manuscript received 21 May; 1993; in revised form 10 August;1993)
引用本文:

谭树松;徐惠彬. 单向、双向记忆合金的相变热测定[J]. 金属学报, 1994, 30(9): 404-408.
, . CALORIMETRIC MEASUREMENTS FOR ONE WAY AND TWO WAY CuZnAl MEMORY ALLOYS[J]. Acta Metall Sin, 1994, 30(9): 404-408.

全文: PDF(373 KB)  
摘要: 用DSC-7研究了CuZnAl单向、双向记忆合金的相变潜热,发现:单向、双向记忆合金相变过程的DSC曲线形状各异,单向记忆合金的DSC曲线为犬牙状,有多个峰;而双向记忆合金的DSC曲线只有一个峰。在相变热的大小上,单向记忆合金的相变热比双向记忆合金约大1/4。
关键词 : CuZnAl,  单向形状记忆合金,  双向形状记忆合金,  相变热    
Abstract:One way and two way shape memory alloys of Cu-21% Zn-6% Al (wt-%)were studied by differential scanning calorimetry. The profiles of endothermic and exothermic peaks of one way shape memory alloy are different from those of two way shape memory alloy.The former shows smooth peaks while the other shows bumpy peaks. Besides, the heat of martensitic transformation of two way shape memory alloy is about 25% less than that of one way shape memory alloy.Correspondent: TAN Shusong, professor, (Department of Materials, Central South University of Technology,Changsha 410083)
Key words: one way memory alloy    two way memory alloy    heat of transformation
收稿日期: 1994-09-18     
1LiuY,MccormickPG.ActaMetallMater,1990;38:13212ContadoL,GueninG.ActaMetallMater,1990;38:12673GueninG.EuropeanconferenceontheMartensiticTransformationinScienceandTechnology.Bochum,FRG,1989:394StalmansR,VanHumbeeckJ,DelaeyL.MaterTransJIM,1992;33:2985ContardoL,GueninG.MaterSciForum,1990;56-58:5296SakamotoH,SugimotoK,NakamuraY,TanakaA,ShimizuK.MaterTransJIM,1991;32:1287XuH,TanS.ScrMetallMater.1991;25:1507
[1] 蒋青. CuAlNi单晶中的DO_3→2H和DO_3→18R转变及其相变热力学[J]. 金属学报, 1994, 30(2): 49-54.
[2] 程饴萱;陈继勤;方晓旻;吕卫平. CuZnAl合金的马氏体及其相变的阻尼性能[J]. 金属学报, 1991, 27(3): 56-60.
[3] 杨全民;康沫狂. 奥氏体贫碳区性质与贝氏体相变热力学[J]. 金属学报, 1990, 26(4): 5-11.
[4] 王世道;俞德刚. Fe-C合金贝氏体相变热力学研究[J]. 金属学报, 1989, 25(4): 23-29.