| 几种纳米固体材料的显微结构特征 |
| 平德海;李斗星;叶恒强;吴希俊 |
| 中国科学院金属研究所固体原子像开放研究实验室;浙江大学 |
|
| ^MICROSTRUCTURE OF NANOCRYSTALLINE MATERIALS |
| PING Dehai; LI Douxing; YE Hengqiang(Laboratory of Atomic Imaging of Solids;Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015). WU Xijun(Zhejiang University; Hangzhou 310014) (Manuscript received 94-06-30) |
引用本文:
平德海;李斗星;叶恒强;吴希俊. 几种纳米固体材料的显微结构特征[J]. 金属学报, 1995, 31(2): 79-84.
,
,
,
.
^MICROSTRUCTURE OF NANOCRYSTALLINE MATERIALS[J]. Acta Metall Sin, 1995, 31(2): 79-84.
| 1MelendresCA,NarayanasamyA,MaroniVA,SiegelRW.J.MaterRes,1989:4:12462FitzsimmonsMR,EastmanJA,Miiller-StachM,WallnerG.PhysRev.1991:44B:24523JorraE,FranzH,PeislJ,WallnerG,PetryW,BirringerR,GleiterH,HauboldT.PhilosMag,1989:60B:1594ZhuX,BirringerR,HerrU,GleiterH.PhysRev,1987;35B:90855HauboldT,BirringerR,LengelerB,GleiterH.PhysLett,1989:135:4616GleiterH.ProgMaterSci,1989;33:2237WunderlichW,IshidaY,MaurerR.SerMetallMater,1990;24:4038SiegelRW,ThomasGJ.Ultramicroscopy,1992,40:3769LiDX,PingDH,YeHQ,QinXY,WuXJ.MaterLett,1993;18:2910YshizawaY,OgumaS,YamauchiKJApplPhys,1988:64:606411LuK,WangJT,WeiWD.JApplPhys,1991;69:52212吴希俊.力学进展,1991.21:6313BirringerR,HerrU,GleiterH.TransJpnInstMet,1986:27(Suppl.):43: |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|