| 基于塑性应变的变幅应力疲劳损伤评估方法 |
| 张继旺;鲁连涛;沈训梁;衣鸿飞;张卫华 |
| 西南交通大学牵引动力国家重点实验室; 成都 610031 |
|
| EVALUATION METHOD OF FATIGUE DAMAGE UNDER VARIABLE AMPLITUDE STRESS BASED ON PLASTIC STRAIN |
| ZHANG Jiwang; LU Liantao; SHEN Xunliang; YI Hongfei; ZHANG Weihua |
| State Key Laboratory of Traction Power; Southwest Jiaotong University; Chengdu 610031 |
引用本文:
张继旺 鲁连涛 沈训梁 衣鸿飞 张卫华. 基于塑性应变的变幅应力疲劳损伤评估方法[J]. 金属学报, 2009, 45(12): 1461-1465.
,
,
,
,
.
EVALUATION METHOD OF FATIGUE DAMAGE UNDER VARIABLE AMPLITUDE STRESS BASED ON PLASTIC STRAIN[J]. Acta Metall Sin, 2009, 45(12): 1461-1465.
| [1] Horikawa T, Nakamura H. Fatigue Strength of Metal and Application to Fatigue Strength Design. Tokyo: coronasha, 2008: 100
(中村宏, 堀川武.金属疲劳の基础と疲劳强度设计への型用, 东京: コロナ社, 2008: 100)
[2] Miner M A. J Appl Mech, 1945; 12A(3): 159
[3] Xu H. Fatigue Strength. Beijing: Higher Education Press,188: 90
(徐灏. 疲劳强度. 北京: 高等教育出版社, 1988; 90)
[4] Ren W X, Huang D X. J Chin Railway Soc, 1991; 6(2): 73
(任伟新, 黄大祥. 铁道学报, 1991; 6(2): 73)
[5] Wang L Y, Peng Z Y. Res Explor Lab, 2007; 26: 1990
(王丽英, 彭忠义. 试验室研究与探索, 2007; 26: 1990)
[6] He Z M, Zhao Y X, Yang B, Gao Q, Wu P B. Eng Mech, 2005; 22: 200
(何朝明, 赵永翔, 杨冰, 高庆, 邬平波. 工程力学, 2005; 22: 200)
[7] Zhao Y X, Hang Y Z, Gao Q. J Traffic Transport Eng, 2003; 3(2): 11
(赵永翔, 黄郁仲, 高庆, 交通运输工程学报, 2003; 3(2): 11)
[8] Beretta S, Carboni M. Eng Fract Mech, 2006; 73: 2627
[9] Basquin O H. Proceedings ASTM, 1919; 10(PartII): 625
[10] Weibll W. Fatigue Testing and Analysis of Results. London: Pergamon Press, 1961: 201
[11] Horikawa T, Nakamura H. J Soc Mater Sci, Jpn, 1973; 23(244): 46
(堀川武, 中村宏. 材料, 1974; 23(244): 46)
[12] Manson S S. Syracuse: Syracuse University Press, 1964:133
[13] Zhao Y X, Yang B, Sun Y F, Gao Q. Chin J Mech Eng, 2004; 40(9): 48
(赵永翔, 杨冰, 孙亚芳, 高庆. 机械工程学报, 2004; 40(9): 48)
[14] Kikukawa M, Ohji K, Kamata T, Jono M. J Jpn Soc Mech Eng, 1967; 70(585): 1495
(菊川真, 大路清嗣, 濂田敬雄, 城野政弘.日本机械学会志, 1967; 70(585): 1495) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|