| Frank-Read位错源的细观级模拟 |
| 余勇; 潘晓霞 |
| 中国工程物理研究院总体工程研究所; 绵阳 621900 |
|
| MESO-SCALE SIMULATION OF FRANK-READ DISLOCATION SOURCES |
| YU Yong; PAN Xiaoxia |
| Institute of System Engineering; China Academy of Engineering Physics; Mianyang 621900 |
引用本文:
余勇 潘晓霞. Frank-Read位错源的细观级模拟[J]. 金属学报, 2009, 45(11): 1309-1313.
,
.
MESO-SCALE SIMULATION OF FRANK-READ DISLOCATION SOURCES[J]. Acta Metall Sin, 2009, 45(11): 1309-1313.
| [1] Bulatov V V. J Comput Aided Mater Des, 2002; 9: 133
[2] Kubin L P. Phys Status Solidi, 1993; 135A: 433
[3] Raabe D. Comput Mater Sci, 1998; 11: 1
[4] Zbib H M, Rabia T D, Rhee M, Hirth J P. J Nucl Mater, 2000; 276: 154
[5] Rhee M, Zbib H M, Hirth J P, Huang H, Rubia T D. Modell Simul Mater Sci Eng, 1998; 6: 467
[6] Zbib H M, Rhee M, Hirth J P. Int J Mech Sci, 1998; 40: 113
[7] Geipel T. Acta Mater, 1997; 45: 2639
[8] Faradjian A K, Friedman L H, Chrzan D C. Modell Simul Mater Sci Eng, 1999; 7: 479
[9] Hirth J P, Lothe J. Theory of Dislocation. New York: John Weiley & Sons, 1982: 133
[10] Cai W, Arsenlis A, Weinbergr C R, Bulatov V V. J Mech Phys Solids, 2006; 54: 561
[11] Yu Y, Pan X X, Rong Y H. Acta Metall Sin (Engl Lett), 2008; 21: 94
[12] Mughrabi H. Mater Sci Eng, 2001; A309–310: 237
[13] Weygand D, Friedman L H, Van der Giessen E, Needlemen A. Modell Simul Mater Sci Eng, 2002; 10: 437
[14] Ghoniem N M, Tong S H, Sun L Z. Phys Rev, 2000; 61B: 913 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|