| 铌基超高温合金表面包埋Si-Y共渗涂层的显微组织 |
| 田晓东;郭喜平 |
| 西北工业大学凝固技术国家重点实验室 |
|
引用本文:
田晓东; 郭喜平 . 铌基超高温合金表面包埋Si-Y共渗涂层的显微组织[J]. 金属学报, 2008, 44(5): 585-588 .
[1]Bewlay B P,Jackson M R,Zhao J C,Subraraanian P R. Metall Mater Trans,2003;34A:2043 [2]Sarath E,Menon K.Mater Sci Forum,2005;475/479:717 [3]Stringer J.Mater Sci Eng,1989;A120:129 [4]Zhai J K,Ma X,Bai X D,Hou W H.Acta Aeronaut As- tronaut Sin,1994;15:499 (翟金坤,马祥,白新德,侯卫红.航空学报,1994;15:499) [5]Wang Y,Gao J P,Li Y P,Hu X F.J lnorg Mater,2000; 15:143 (王禹,郜嘉平,李云鹏,胡行方.无机材料学报,2000;15:143) [6]Li M,Song L X,Le J,Song X P,Guo Z C.J Inorg Mater, 2005;20:764 (李明,宋力昕,乐军,宋学平,郭占成.无机材料学报,2005;20:764) [7]Bianco R,Harper M A,Rapp R A.JOM,1991;43(11):68 [8]Fernandes P B,Coelho G C.Intermetallics,2002;10:993 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|