B元素对Ti-46Al和Ti-46Al-5Nb合金柱状晶组织的影响
杨慧敏;苏彦庆;郭景杰;骆良顺;李新中;傅恒志
Effects of B addition on the columnar structures of Ti-46Al and Ti-46Al-5Nb alloys
YANG Hui-Min
哈尔滨工业大学
引用本文:

杨慧敏; 苏彦庆; 郭景杰; 骆良顺; 李新中; 傅恒志 . B元素对Ti-46Al和Ti-46Al-5Nb合金柱状晶组织的影响[J]. 金属学报, 2008, 44(10): 1213-1218 .
, , , , , . Effects of B addition on the columnar structures of Ti-46Al and Ti-46Al-5Nb alloys[J]. Acta Metall Sin, 2008, 44(10): 1213-1218 .

全文: PDF(3420 KB)  
摘要: B元素对Ti-46Al和Ti-46Al-5Nb(原子分数, %)合金的柱状晶组织均有明显的细化作用, 且对后者的细化效果更显著. 这一现象可归结为: B元素在Ti-46Al-5Nb合金中 的溶解度较低, 硼化物析出量增加, 柱状晶组织进一步细化.
关键词 : B添加,  Ti-46Al,  Ti-46Al-5Nb    
Abstract:The effects of B content on the columnar structures of unidirectionally solidified Ti-46Al and Ti-46Al-5Nb alloys were investigated in the paper. The results show that, with B addition, the columnar structures of Ti-46Al and Ti-46Al-5Nb alloys are refined. The effect of B addition on the columnar structure refinement of Ti-46Al-5Nb alloy is greater than that of Ti-46Al alloy. This is resulted from two reasons. (1) The effects of Nb addition on the columnar structure refinement of Ti-46Al alloy. (2) In Ti-46Al alloy the boride fraction is increased because the solubility of B element was decreased with Nb addition.
Key words: B    Ti-46Al    Ti-46Al-5Nb    columnar structure
收稿日期: 2008-02-26     
ZTFLH:  TG146.4  
[1]Dimiduk D M.Mater Sci Eng,1999;A263:281
[2]Jung I S,Jang H S,Oh M H,Lee J H,Wee D M.Mater Sci Eng,2002;A329-331:13
[3]Yamaguchi M,Johnson D R,Lee H N,Inui H.Inter- metallics,2000;8:511
[4]Lu Y H,Zhang Y G,Qiao L J,Wang Y B,Chen C Q,Chu W Y.Acta Metall Sin,1999;35:1233 (陆永浩,张永刚,乔利杰,王燕斌,陈昌麒,褚武扬.金属学报,1999;35:1233)
[5]Zhang J,Zhang Z H,Zou D X,Zhong Z Y.Acta Metall Sin,1996;32:1044 (张继,张志宏,邹敦叙,仲增墉.金属学报,1996;32:1044)
[6]Hu D.Intermetallics,2001;9:1037
[7]Dong L M,Cui Y Y,Yang R.Acta Metall Sin,2002;38: 643 (董利民,崔玉友,杨锐.金属学报,2002;38:643)
[8]Cheng T T.Intermetallics,2000;8:29
[9]Rao G B,Liu K,Han E H,Ke W.Chin d Nonferrous Metals,2004;14(Suppl.1):265 (饶光斌,刘奎,韩恩厚,柯伟.中国有色金属学报,2004;14(专辑1):265)
[10]Larson D J,Liu C T,Miller M K.Mater Sci Eng,1997; A239-240:220
[1] 魏世同 陆善平 何广忠 赵旭 李殿中 李依依. 热处理工艺对含Nb焊缝金属组织与力学性能的影响[J]. 金属学报, 2009, 45(9): 1063-1069.
[2] 魏伟; 单以银; 杨柯; 王永权 . 添加Mo-B对超高强度管线钢相变组织的影响[J]. 金属学报, 2007, 43(9): 943-948 .