BaCe1-xYxO3-α及BaCe0.9Sm0.1O3-α质子导体的性能表征及组成氢泵对Al熔体脱氢的研究
王 东 范建华 刘春明 王常珍
东北大学材料与冶金学院
Characteristics of Proton Conductors BaCe1-xYxO3- and BaCe0.9Sm0.1O3- and Dehydrogenation of Al Melt with Composed Hydrogen Pump
WANG Dong; FAN Jianhua; LIU Chunming; WANG Changzhen
College of Materials and Metallurgy; Northeastern University
引用本文:

王东; 范建华; 刘春明; 王常珍 . BaCe1-xYxO3-α及BaCe0.9Sm0.1O3-α质子导体的性能表征及组成氢泵对Al熔体脱氢的研究[J]. 金属学报, 2007, 43(11): 1228-1232 .
, , , . Characteristics of Proton Conductors BaCe1-xYxO3- and BaCe0.9Sm0.1O3- and Dehydrogenation of Al Melt with Composed Hydrogen Pump[J]. Acta Metall Sin, 2007, 43(11): 1228-1232 .

全文: PDF(853 KB)  
摘要: 采用固相合成法制备了BaCe0.9Y0.1O3-α、BaCe0.85Y0.15O3-α和BaCe0.9Sm0.1O3-α质子导体。X射线衍射(XRD)结果表明掺10%Y的物料形成了纯净的钙钛矿型固溶体;而掺15%Y的物料不含Y2O3,主相为钙钛矿型固体电解质。据此推断,Y在BaCeO3中的固溶度极限大于0.15。掺10%Sm物料的XRD谱未显示有Sm2O3存在,因此Sm在BaCeO3的固溶度极限大于0.10。激光散射粒度分析结果表明合成后粉体颗粒的平均粒径变大,粒径5μm左右的颗粒所占比例最高。TG-DSC分析表明质子导体的合成温度为1360℃。扫描电镜(SEM)的结果显示,质子导体由分布均匀的大小两种颗粒构成,颗粒尺寸在1μm—10μm之间。BaCe0.9Y0.1O3-α和BaCe0.9Sm0.1O3-α脱氢电池对铝液的脱氢结果表明,脱氢电流随着铝液温度的升高,水蒸气压的增大,外加电压的增加而依次增大。用自制的CaZr0.9In0.1O3-α测氢传感器测得铝液温度780℃,水蒸气压为4122.8Pa和4366.0Pa时铝液中的氢活度分别为0.0536和0.0445 mlH2/100gAl。
关键词 : BaCe1-xYxO3-α,  BaCe0.9Sm0.1O3-α,  质子导    
Abstract:BaCe0.9Y0.1O3-α,BaCe0.85Y0.15O3-α and BaCe0.9Sm0.1O3-α proton conductors were prepared by solid state reaction. X-ray Diffraction(XRD) indicated the powders doped 10%Y were single perovskite phase. The powders doped 15%Y and 10%Sm didn`t have Y2O3 and Sm2O3 respectively. It was concluded that solid sulubility limit of Y is above 0.15 and that of Sm is above 0.10 in BaCeO3. By laser light scattering paticle size analysis indicated that average particle size of powders changed larger and particles that particle size is about 5μm accounted for the most quantitatively after calcination. TG-DSC analysis displayed the sintering temperature of proton conductors was about 1360℃. SEM showed these proton conductors were composed of two particles whose size ranged from 1μm to 10μm. The Dehydrogenation result indicated deydrogenation current getted higher when the temperature of Al melt,water vapor pressure and external voltage getted higher independently. By CaZr0.9In0.1O3-α hydrogen sensor the hydrogen activity was 0.0536 and 0.0445 mlH2/100gAl when the temperature of Al melt was 780℃, PH2O was apart 4122.8Pa and 4366.0Pa.
Key words: BaCe1-xYxO3-α    BaCe0.9Sm0.1O3-α    proton conductor    hydrogen pump    dehydrogenation of Al melt
收稿日期: 2007-02-12     
ZTFLH:  O646  
[1]Iwahara H,Esaka T,Uchida H,Maeda N.Solid State Ion- its,1981;3/4:359
[2]Iwahara H,Uchida H,Tanaka S.Solid State lonics,1983; 9/10:1021
[3]Mitsui A,Miyayama M,Yanagida H.Proc 3rd Meeting on Chemical Sensors,Tokyo,Japan:1984
[4]Iwahara H,Uchida H,Ono K,Ogaki K.J Electrochem Soc,1988;135:529
[5]Hibino T,Mizutani K,Yajima T,Iwahara H.Solid State Ionics,1992;57:303
[6]Iwahara H,Esaka T,Uchida H,Yamauchi T,Ogaki K. Solid State Ionics,1986;18/19:1003
[7]Iwahara H,Uchida H,Nagano T,Koide K.Denki Kagaku, 1989;57:992 (岩原弘育,内田裕之,长野贵小,出邦博.电气化学,1989;57:992)
[8]Iwahara H,Uchida H,Morimoto K.Denki Kagaku,1990; 58:178 (岩原弘育,内田裕之,森木清幸.电气化学,1990;58:178)
[9]Iwahara H.Solid State Ionics,1992;52:99
[10]Iwahara H.Solid State Ionics,1995;77:289
[11]Hibino T,Hashimoto A,Suzuki M,Sano M.J Electrochem Soc,2002;149:A1503
[12]Gokcen N A,Chipman J.Trans AIME,1952;194:171
[13]Zhou G D.Dictionary of Chemistry.Beijing:Chemical Industry Press,2004:670 (周公度.化学辞典.北京:化学工业出版社,2004:670)
[14]Yang N R,Yue W H.The Handbook of Inorganic Metal- loid Meterials Atlas.Wuhan:Wuhan University of Tech- nology Press,2000:213 (杨南如,岳文海.无机非金属材料图谱手册.武汉:武汉工业大学出版社,2000:213)
[1] 厉英,丁玉石,崔绍刚,王常珍. 掺杂Sc的CaZrO3的制备及电学性能[J]. 金属学报, 2012, 48(5): 575-578.
[2] 厉英 丁玉石 胡井涛 王常珍. 用质子导体传感法研究钢在脱氢热处理中氢的行为[J]. 金属学报, 2011, 47(5): 553-558.
[3] 王东 刘春明 王常珍. 高温质子导体Ba3Ca1.18Nb1.82O9-δ的制备和表征[J]. 金属学报, 2009, 45(3): 345-350.
[4] 郑敏辉;陈祥. SrCeO_3基高温质子导体及Al液定氢探头[J]. 金属学报, 1994, 30(17): 238-242.