| 金属直薄壁件激光直接沉积过程的有限元模拟 III. 沉积过程中变形的分析 |
| 高士友; 石力开; 席明哲; 纪宏志; 张永忠; 杜宝亮 |
| 北京有色金属研究总院 |
|
| Finite Element Simulation for Laser Direct Depositing Processes of Metallic Vertical Thin Parts(3) |
引用本文:
高士友; 石力开; 席明哲; 纪宏志; 张永忠; 杜宝亮 . 金属直薄壁件激光直接沉积过程的有限元模拟 III. 沉积过程中变形的分析[J]. 金属学报, 2006, 42(5): 459-462 .
[1] Hofmeister W H, Bayuzick R J, Robinson M B. Int J Thermophys, 2000; 10(1): 279 [2] Jendrzejewski R, Kreja I, Sliwiriski G. Mater Sci Eng, 2004; A379: 313 [3] Hu D, Kovacevic R S. Int J Mach Tool Manuf, 2003; 43: 51 [4] Toyserkani E, Khajepour A, Corbin S. Opt Laser Eng, 2004; 41: 849 [5] Brockmann R, Dickmann K. Opt Laser Technol, 2003; 35: 115 [6] Hofmeister W, Griffith M, Ensz M, Smugeresky J. JOM, 2001; 53(9): 30 [7] Shawn M K. Master Thesis. Virginia Polytechnic Institute and State University, 2002 [8] Nickel A H. PhD Thesis, Stanford University, 1999 [9] Nickel A H, Barnett D M, Prinz F B. Mater Sci Eng, 2001; A317: 59 [10] Labudovic M, Hu D, Kovacevic R. J Mater Sci, 2003; 38: 35 [11] Shen Z H, Zhang S Y. Opt Laser Technol, 2001; 33: 533 [12] Dai K, Shaw L. Acta Mater, 2004; 52: 69 [13] Shi L K, Gao S Y, Xi M Z, Ji H Z, Zhang Y Z, Du B L. Acta Ueiall Sin, 2006; 42: 449 (石力开,高士友,席明哲,纪宏志,张永忠,杜宝亮.金属学 报,2006;42:449) [14] Shi L K, Gao S Y, Xi M Z, Ji H Z, Zhang Y Z, Du B L. Acta Metall Sin, 2006; 42: 454 (石力开,高士友,席明哲,纪宏志,张永忠,杜宝亮.金属学 报,2006;42:454) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|